A Study on Behavior of Oxide Inclusions in Bearing Steel GCrl5 at Refining End of a 60t LF
With the deoxidation by adding ferroaluminium and ferrosilicon in EAF tapping and the LF initial refining slag (/%:27.39~37.34 Al2O338.42~38.68 CaO,14.20~18.38 SiO28.50~10.72 MgO,0.82~0.89 FeO,0.27~0.33 MnO,0.69~0.74 S,0.66~0.75TiO2(CaO)/(SiO2)=2.09~2.72,
沈万林, 张志成, 罗小燕
doaj
The electroslag-remelting (ESR) test on steel Cr13Mn4Mo by 70CaF2-30Al2O3slag series has been carried out. The total oxygen content, sulfur content and amount, size and morphology of inclusions in Ф55mm electrode and Ф120mm (36kg) ESR ingot are analyzed ...
张钊 +5 more
doaj
Evolution of Inclusions in High Quality Medium Steel Plates during Steelmaking Process [PDF]
Jingxin DAI +5 more
core +1 more source
Evolution of Inclusions in Steel with 150 t LF Refining Feeding Calcium Wire Treatment
The evolution of inclusions in steel Q235, SPA-H and DC01 treated by feeding silicon-calcium wire and calcium-aluminium wire after LF refining in metal pretreatment-150 t BOF-ladle argon blowing-LF-CSP flowsheet and the effect of refining slag on ...
姜玉龙 +6 more
doaj
Analysis and Control of Inclusions in Steel for High Pressure Boiler Tubes [PDF]
Baojian KONG +4 more
core +1 more source
Evolution of Inclusions in Gear Steel 18CrNiMo7-6 during 60t LF-VD Reflning Process
The metallurgical flowsheet for steel 18CrNiMo7-6 (/%: 0. 17C, 0. 57Mn, 0. 24Si, 0. 012P, 0. 003S, 1.70Cr, 1. 49Ni, 0. 28Mo) is 60t EAF-LF-VD-2.1t ingot.
刘金鑫 +4 more
doaj
Analysis of Bridge Steel Plate Flaw Detection Disqualification [PDF]
Hao WANG +5 more
core +1 more source
[Surgical robot-assisted submandibular gland excision through retroauricular hairline approach: three case reports]. [PDF]
Ma S, He J, Cao C, Wang X, Li C, Zhu G.
europepmc +1 more source
Weld Cracking Analysis of SPHT1 High Frequency Welded Pipe [PDF]
Chongtao SU, Haixia ZUO, Xiaojing GUO
core +1 more source