Results 21 to 30 of about 160,422 (158)
本文用三点弯曲和四点弯曲试样,在K_Ⅱ/K_Ⅰ=0—14的范围内,对GC-4超高强度钢、30Cr2MoV中强度转子钢和稀土球墨铸铁进行了线弹性平面应变复合型脆断试验。结果表明:复合型裂纹的脆断开裂方向与现有的三种复合型理论符合较好;但是,复合型裂纹扩展阻力随K_Ⅱ/K_Ⅰ比值增加而增大,与现有复合型理论差别较大。本文从塑性区的形状、大小和裂纹顶端在开裂方向的应力状态等方面对此问题进行了分析并指出,现有理论关于复合型裂纹扩展阻力与变形特征无关的假设,对于具有一定塑性变形能力的金属材料,是不合适的 ...
杨成寿, 王自强, 高桦, 周爱华
core +2 more sources
针对一起500 kV断路器爆破片破裂事故,通过对破裂爆破片开展理化检验,发现故障爆破片材质为灰铸铁,表面有微孔,双侧用橡胶层密封保护,没有锈蚀,电镜分析表明材料脆性较大。通过更换同型断路器爆破片,比较新旧爆破片的性能,发现旧爆破片均有变形,大部分旧爆破片外侧橡胶层老化龟裂,导致爆破片进水锈蚀。通过开展爆破试验,发现部分旧爆破片爆破压力降低,但并不是锈蚀严重的样品。结果表明锈蚀并不是导致爆破片爆破压力下降的关键原因,该爆破片为平板型,铸铁材质,脆性较大,抗疲劳性能不足 ...
焦宗寒, 郑欣, 马宏明, 宋玉锋
doaj
ABSTRACT Biodegradable magnesium alloys are limited in orthopedic applications due to their rapid corrosion and poor interfacial stability. In this work, a composite coating is constructed via magnetic filtered cathodic vacuum arc (MFCVA) deposition of a Zn interlayer, followed by hydrothermal in situ generation of ZnO to induce hydroxyapatite (HA ...
Chao Zhang +9 more
wiley +1 more source
ABSTRACT Carbides strengthen the grain boundaries; nevertheless, excessive carbide precipitates embrittle the grain boundaries of high‐temperature alloys during prolonged service. Here, we provide direct evidence of solute rare‐earth atoms and demonstrate that they can trap vacancies and inhibit interstitial diffusion, restraining carbide precipitation
Jiali Zhang +10 more
wiley +1 more source
复合绝缘子断串及芯棒击穿事故会对输电线路的安全稳定运行构成严重的威胁。文中对2016年以来浙江省内发生的复合绝缘子断串及芯棒击穿故障案例进行统计分析,包括故障概况、产品情况、故障形态、性能试验、故障原因以及相关建议措施等。结果表明,2016年以来浙江省内共发生8起复合绝缘子断串及芯棒击穿故障,包括6起酥朽断裂、1起脆性断裂及1起芯棒击穿。其中,脆性断裂主要为端部密封不良,外部潮气进入,并在长期高场强作用下产生的应力腐蚀所致;酥朽断裂主要为芯棒—护套粘接不良,在受潮、放电 ...
周晨 +5 more
doaj
ABSTRACT Bimetallic structures fabricated by laser powder bed fusion (LPBF) provide an effective strategy for achieving multifunctional integration, yet interfacial structural continuity and the role of lattice defects remain insufficiently understood.
Jinguo Ge, Shuo Yin
wiley +1 more source
ABSTRACT An ultra‐high as‐deposited tensile strength of 1408 MPa—the highest reported value for laser‐directed energy deposition (L‐DED) fabricated Ti2AlNb alloy—is achieved in this study. The as‐deposited microstructure consists of coarse B2 grains with a high density of fine acicular O phase precipitates within the grains, along with a brittle α2 ...
Ximiao He +7 more
wiley +1 more source
介绍了一起复合绝缘子脆断的发生过程,通过解剖和相关电气、机械性能试验,以及脆断面形成机理等方面分析了脆断原因,发现芯棒脆断的原因是运行环境的恶劣加之结构的缺陷使得端部密封不良,造成酸蚀并最终导致芯棒机械性能下降而发生脆断。为防止脆断事故的发生,从加强检验、连接方式、材料工艺、存储安装等方面提出了相应的对策,保证电网的安全可靠运行。
郭清滔, 廖福旺, 黄海鲲
doaj
Simulating hydrogen embrittlement fracture based on phase field method
The phase field hydrogen embrittlement fracture model is improved by introducing tension-compression split of strain energy. The numerical formulas of the model are provided, besides, the coupling term of concentration field and displacement field is ...
CHEN Pengcheng +3 more
doaj +1 more source