Results 11 to 20 of about 92,077,270 (62)
Impact of a multi-step heat treatment on different manufacturing routes of 18CrNiMo7-6 steel [PDF]
Effect of an optimized multi-step heat treatment routine on conventional (machining from wrought bar stock) and alternate manufacturing routes (hot forging and cold rotary forging) for producing flat cylindrical-shaped machine drive components from ...
Olasolo, Maider +3 more
core +3 more sources
Simulation and Mechanical Properties of Fine-Grained Heat-Affected Zone Microstructure in 18CrNiMo7-6 Steel [PDF]
Heat-affected zones (HAZs) in real welds are usually quite narrow, and consequently most standard mechanical tests are difficult or even impossible. Therefore, simulated microstructures are often used for mechanical tests.
Bjelajac, Edvard +9 more
core +1 more source
The present study is conducted with a dual-aim; firstly, examine the effect of several single shot peening conditions on the subsurface layer properties and fatigue performance of the case-hardened 18CrNiMo7-6 steel.
Penghui Niu +4 more
core +2 more sources
Bending Fretting Fatigue Characteristics of 18CrNiMo7-6 Alloy Steel
A series of bending fretting fatigue tests of 18CrNiMo7-6 alloy steel were carried out, the bending fretting fatigue S-N curve was built up, and an analysis was made on the test results.
PENG Jin-fang +5 more
core +1 more source
BANDED MICROSTRUCTURE IN FORGED 18CrNiMo7-6 STEEL
18CrNiMo7-6 steel, after hot forging, exhibits a distinct banding of ferritic-pearlitic microstructure, probably related to the segregation of alloying elements during the ingot crystallization.
Pawłowski, Bogdan +2 more
core +1 more source
Study on Inclusions Distribution and Cyclic Fatigue Performance of Gear Steel 18CrNiMo7-6 Forging
The three-dimensional morphologies of inclusions in gear steel 18CrNiMo7-6 forging were investigated by a non-destructive extraction method, and the cleanliness of radial positions was analyzed, mainly including the variation of total oxygen content and ...
Wei Xiao +4 more
core +1 more source
Hard milling of carburized and waterjet peened 18CrNiMo7-6 steel
Post-mixed waterjet peening is an effective treatment method for compressive residual stress field. After peening, the surface quality of the parts is low, and the hardness is usually higher than 60HRC.
Ma, Yongtao +9 more
core +1 more source
JoshUoM/Steel-CCT-Predictor: Low Alloy Steel CCT Predictor
CCT predictor for low alloy ...
Joshua Collins
core +1 more source
Abrasive waterjet peening (AWJP) as an important surface strengthening method can effectively improve surface properties. In this study, after multiple AWJP, the distribution of compressive residual stress and roughness on the surface of 18CrNiMo7-6 ...
Yafeng Xu +5 more
core +1 more source
Quenching and partitioning - a new steel heat treatment concept [PDF]
Steel continues to be one of the primary materials in use today, however, even after 200 years of published research, innovative methods are being discovered and exploited to produce steel with enhanced properties.
Bigg, Timothy David
core +5 more sources