Results 11 to 20 of about 481,866 (292)

Dynamic heterogeneity in amorphous materials [PDF]

open access: yesPhysics, 2010
Amorphous solids are mechanically rigid while possessing a disordered structure similar to that of dense liquids. Recent research indicates that dynamical heterogeneity, spatio-temporal fluctuations in local dynamical behavior, might help understanding ...
L. Berthier, Ludovic Berthier, W. Götze
core   +3 more sources

Learning to manipulate amorphous materials [PDF]

open access: yesACM Transactions on Graphics, 2020
We present a method of training character manipulation of amorphous materials such as those often used in cooking. Common examples of amorphous materials include granular materials (salt, uncooked rice), fluids (honey), and visco-plastic materials (sticky rice, softened butter).
Yunbo Zhang   +4 more
openaire   +2 more sources

Amorphous-crystalline Ni-Fe powder mixture: Hydrogenation and annealing effects on microstructure and electrical and magnetic properties [PDF]

open access: yesScience of Sintering, 2016
The hydrogenation of a crystalline Ni-Fe (80 wt.% Ni, 20 wt.% Fe) powder mixture leads to the formation of a mixture of Face Centered Cubic (FCC)-Ni and FCC-Fe phase nanocrystals embedded in an amorphous matrix.
Milinčić Radovan   +4 more
doaj   +1 more source

Effect of deposition current density and annealing temperature on the microstructure and magnetic properties of nanostructured Ni-Fe-W-Cu alloys [PDF]

open access: yesScience of Sintering, 2019
Ni-Fe-W-Cu alloy powders were obtained by electrodeposition from an ammonium citrate bath at current densities ranging between 70 and 600 mA cm-2. As the deposition current density increased, the contents of Fe and W in the alloy increased, and ...
Spasojević Milica   +5 more
doaj   +1 more source

Characterization of FeCoV alloy processed by PIM/MIM route [PDF]

open access: yesScience of Sintering, 2017
In this study the characterization of FeCo-2V alloys toroidal samples produced by PIM/MIM technology was presented. The feedstock for metal injection molding (MIM) was prepared by mixing starting FeCoV powder with a low viscosity binder.
Nedeljković Borivoje   +4 more
doaj   +1 more source

Morphological, microstructural and magnetic characteristics of electrodeposited Ni-Fe-W-Cu alloy powders [PDF]

open access: yesScience of Sintering, 2020
Nanostructured Ni-Fe-W-Cu alloy powders were electrodeposited from an alkaline ammonium citrate solution on a titanium cathode. Powder particles were dendrite- and cauliflower-shaped.
Spasojević Miroslav   +4 more
doaj   +1 more source

The thermal and magnetic properties of the Fe89.8Ni1.5Si5.2B3C0.5 and Fe81B13Si14C2 amorphous alloys [PDF]

open access: yesScience of Sintering, 2015
This paper investigates the thermal and magnetic properties of two iron based amorphous alloys with different Fe-content: Fe89.8Ni1.5Si5.2B3C0.5 and Fe81B13Si14C2.
Kalezić-Glišović A.   +2 more
doaj   +1 more source

Effect of Solvent and Catalyst Types on Stability and Properties of Zinc Phthalocyanine in the Organic–Inorganic Hybrid Materials

open access: yesCrystals, 2021
Hybrid materials, i.e., the organically modified silicates (ORMOSIL) based on zincphthalocyanine (ZnPc) and silica glass matrix were synthesized by the sol-gel method using protic solvents (methanol, ethanol, isopropanol, butanol) and aprotic solvent (N ...
Barbara Popanda   +2 more
doaj   +1 more source

The inverted hysteresis loops and exchange bias effects in amorphous/nanocrystalline Fe72Cu1V4Si15B8 ribbons at room temperature [PDF]

open access: yesScience of Sintering, 2020
Тhe influence of thermally induced microstructural transformations on magnetic properties of Fe72Cu1V4Si15B8 ribbon with combined amorphous/nanocrystalline structure is presented.
Surla Radoslav   +3 more
doaj   +1 more source

Synthesis, structure and properties of nickel-iron-tungsten alloy electrodeposits - Part II: Effect of microstructure on hardness, electrical and magnetic properties [PDF]

open access: yesScience of Sintering, 2016
Nanostructured nickel-iron-tungsten alloys were produced by electrodeposition from an ammoniacal citrate bath. The tungsten content of the alloy ranged from 0.8 wt.% to 11 wt.%, and the crystal grain size of the FCC phase of the solid solution ...
Ćirović Nataša   +5 more
doaj   +1 more source