Results 151 to 160 of about 150,466 (305)

Dimercaprol (BAL): Insights into conformational stability, fragmentation pathways via tandem LR-ESI, HR-EI mass spectrometry, and gas-phase thermochemical properties from quantum chemical calculations. [PDF]

open access: yesPLoS One
Molano MF   +9 more
europepmc   +1 more source

Failure Investigation of Alloy 625 Sockolets After Prolonged Service in an Ammonia Cracker Unit

open access: yesMaterials and Corrosion, EarlyView.
The failure of the sockolets was caused by intergranular cracking and fracture. The thick and highly brittle nitrided layer formed intergranular surface cracks, which propagated along grain boundaries into the base alloy substrate due to the presence of brittle Cr‐rich carbides. ABSTRACT Several sockolets of Alloy 625 operating at 540°C in contact with
Kamlesh Chandra   +2 more
wiley   +1 more source

Experimental and Comparative Study of the Corrosion Behavior of Lean Duplex Stainless Steel in Seawater

open access: yesMaterials and Corrosion, EarlyView.
The localized corrosion behavior of lean duplex stainless steel EN 1.4062 is systematically compared with austenitic and higher‐alloyed duplex grades in natural seawater. A clear resistance ranking is established, highlighting EN 1.4062 as a cost‐effective alternative for limited marine exposure.
Mohammad Hassanzadeh   +4 more
wiley   +1 more source

Corrosion Inhibition of S275 Carbon Steel in CO2 Capture Systems Using Monoethanolamine (MEA) Solvent

open access: yesMaterials and Corrosion, EarlyView.
Corrosion inhibitors CuSO4 and NaVO3 achieved up to 98% inhibition efficiency for carbon steel S275 in CO2‐loaded MEA solvent, reducing corrosion rates to 9.4 µm/year—outperforming costly stainless steel SS 316 L at a fraction of the cost. ABSTRACT Corrosion in CO2 capture units significantly impacts safety and costs.
Eleni Lamprou   +6 more
wiley   +1 more source

Hattmakarens bal

open access: yes, 2018
Affisch för teaterföreställningen Hattmakarens bal på Åbo Svenska Teater 1.1 ...
Kinmanson (Kinmansson), Selfrid
core  

Corrosion Behavior of Commercial FeCrAl and TiAl Alloys in Molten Pb With 2E‐7 wt% Oxygen at 600°C and 700°C

open access: yesMaterials and Corrosion, EarlyView.
Excellent corrosion resistance of commercial Al‐containing materials is shown for exposures to liquid lead (Pb) at 600°C. However, oxide scale failure occurs at 700°C. The formed oxide scales and their failure mechanisms are explored. ABSTRACT Liquid lead (Pb) is an attractive heat transfer fluid for advanced thermal energy storage (TES) systems.
Renate Fetzer   +4 more
wiley   +1 more source