Flexural Behavior of 3D‐Printed Porous Bouligand‐Structured Polymers: Influence of Pitch Angle and Porosity

open access: yesAdvanced Engineering Materials, EarlyView.
This study examines how helicoidal architectures with different porosities respond to bending. Adjusting layer angle and spacing in 3D‐printed polymers reveals clear tradeoffs between stiffness, strength, and energy absorption. Experiments and simulations highlight designs that distribute stress effectively, offering pathways for optimizing lightweight
Praveenkumar Subhash Patil   +2 more
wiley   +1 more source

The dynamic response of Pine Island Glacier to two decades of intermittent ice shelf regrounding. [PDF]

open access: yesNat Commun
Surawy-Stepney T   +5 more
europepmc   +1 more source

Density Measurement of Irradiated and Nonirradiated Zirconium Oxide by Ptychographic X‐Ray Computed Tomography (PXCT)

open access: yesAdvanced Engineering Materials, EarlyView.
Mass density governs the protective behavior of oxide layers on nuclear fuel cladding. Ptychographic X‐ray computed tomography measures zirconium oxide grown on Zircaloy‐4 under reactor and autoclave conditions, revealing nearly identical bulk densities of 5.1 ± 0.80 g cm−3.
Okan Yetik   +9 more
wiley   +1 more source

Revisiting estimates of diffuse contamination of agricultural soils by Pb. [PDF]

open access: yesEnviron Monit Assess
Matys Grygar T   +7 more
europepmc   +1 more source

Electrochemical Behavior of Flame‐Sprayed Sc‐Doped AlCoCrFeMo High‐Entropy Alloy Coatings in 3.5% Sodium Chloride Solution

open access: yesAdvanced Engineering Materials, EarlyView.
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar   +7 more
wiley   +1 more source

Distinct Microstructural Characteristic Lengths Defining Notch Fatigue Crack Initiation and Propagation, and Defect Tolerance in Advanced Steels

open access: yesAdvanced Engineering Materials, EarlyView.
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas
wiley   +1 more source

Investigating the Effect of Inclination Angle and the Influence of Scan Parameters on the Appearance and Thermal and Mechanical Properties of Filigree Tension Rods of LPBF‐Manufactured NiTi Shape‐Memory Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
This article investigates the dependence of the properties on the manufacturing orientation in the form of the inclination angle to the build plate of LPBF‐fabricated NiTi rods with a diameter of 150–220 µm. Metallographic, chemical, thermal, and mechanical characterization show behavior under identical manufacturing conditions that ranges from ...
Sandra Herzig   +2 more