Results 141 to 150 of about 29,126 (284)
Orbital pacing of environmental perturbations in a Greenhouse World: a 40-Myr record from Upper Devonian-Lower Carboniferous successions on the eastern margin of Gondwana. [PDF]
Falahatkhah O +4 more
europepmc +1 more source
Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi +5 more
wiley +1 more source
Unsteady Creep Damage Model of Rock Considering Acid Solution Corrosion. [PDF]
Lv H.
europepmc +1 more source
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas
wiley +1 more source
The thorax of <i>E</i> <i>ubleptus</i> illuminates evolutionary history of winged insects. [PDF]
Prokop J +3 more
europepmc +1 more source
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt +5 more
wiley +1 more source
Reply to Discussion by R. A. Henderson of 'Kinematics of the Clarke River Shear Zone (northeastern Australia) and implications for the tectonic evolution of the Tasmanides'. [PDF]
Rodrigues RT, Rosenbaum G.
europepmc +1 more source
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...
Sameh Dabees +6 more
wiley +1 more source
Early sarcopterygian morphological disparity through the Devonian-Carboniferous crisis. [PDF]
Vanhaesebroucke O +2 more
europepmc +1 more source