Low-temperature tempering of carburized and hardened steel 30KhGT
Metal Science and Heat Treatment of Metals, 19591. The optimum tempering conditions of steel 30KhGT are 180°–200° C for 90 minutes' holding. 2. The impact toughness of such steel case-hardened to a 1.1–1.2 mm depth by carburizing and tempered at 120°–150° C/90 min. is by 20%–40% less than that obtained for the optimum tempering conditions. 3.
openaire +1 more source
The Development of in-8000 — a Carburization Resistant High Temperature Alloy
CORROSION 1984, 1984Abstract Ethylene production by pyrolysis, coal gasification, and generation of process heat from high temperature nuclear reactors for direct iron ore reduction, cement making and other thermally intensive processes will require in the future alloys beyond the capabilities of HK-40 and all other commercially available alloys.
openaire +1 more source
Carburization susceptibility of chromia-forming alloys in high-temperature CO2
Corrosion Science, 2022Richard P. Oleksak +3 more
openaire +1 more source
Low Temperature Carburizing of Stainless Steels and the Development of Carbon Expanded Austenite*
HTM - Journal of Heat Treatment and Materials, 2022T L Christiansen, M A J Somers
exaly
High-temperature ionic carburization
Metal Science and Heat Treatment of Metals, 1961openaire +1 more source
AISI 420 martensitic stainless steel low-temperature plasma assisted carburizing kinetics
Surface and Coatings Technology, 2013C J Scheuer +2 more