Results 41 to 50 of about 5,711 (118)
Development and Characterization of an Electrically Rechargeable Zinc-Air Battery Stack
An electrically rechargeable zinc-air battery stack consisting of three single cells in series was designed using a novel structured bipolar plate with air-breathing holes.
Hongyun Ma +3 more
doaj +1 more source
The intrinsic charge‐induced surface stress of Ni thin films during electrochemical reactions with an alkaline electrolyte is measured in situ. Surface stresses induced by H absorption/desorption, α‐Ni(OH)2 formation, capacitive double‐layer charging ...
Chuan Cheng +2 more
doaj +1 more source
Anisotropic hydrogen embrittlement behavior of hot-rolled A572 steel
In the present work, an investigation of the susceptibility to hydrogen embrittlement of a hot rolled ASTM A572 steel with a banded pearlite/ferrite microstructure was conducted, with the objective of elucidating the anisotropic mechanical behavior of ...
Paulo Henrique Barbosa +4 more
doaj +1 more source
Modeling current density and SoC distribution of all-solid-state lithium-ion batteries
Researchers have conducted in-depth investigations into lithium-ion battery models. However, a notable limitation of existing models lies in the assumption of infinitely conductive current collectors, which compromises simulation accuracy.
Zhenya Wang +7 more
doaj +1 more source
In this paper, it has been demonstrated that compressive residual stress induced by cavitation peening which is one of the mechanical surface modification techniques can reduce invasion of the surface of austenitic stainless steel by hydrogen. Cavitation
Osamu Takakuwa, Hitoshi Soyama
doaj +1 more source
The resource utilization of urea wastewater is an important issue in the environmental field. In the present work, urea can be used as the resource of pure hydrogen production by a temporally decoupled rechargeable metal‐urea battery. During the cathodic
Dong Lv +4 more
doaj +1 more source
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging ...
Laurence Latu-Romain +6 more
doaj +1 more source
Hydrogen-assisted fatigue crack growth in ferritic steels – a fractographic study
Fatigue crack growth (FCG) behavior of a Fe-3wt.%Si ferritic alloy under different environmental conditions using in-situ electrochemical (cathodic) hydrogen (H) charging has been investigated. Three frequencies have been applied.
Wan Di +3 more
doaj +1 more source
Investigation of Hydrogen Embrittlement Susceptibility and Fracture Toughness Drop after in situ Hydrogen Cathodic Charging for an X65 Pipeline Steel. [PDF]
Kyriakopoulou HP +6 more
europepmc +1 more source
Advanced high-strength steels (AHSS) are susceptible to edge fracture and hydrogen embrittlement, particularly when both occur simultaneously. This work proposes a novel methodology for evaluating hydrogen embrittlement susceptibility at sheared edges by
Rafael Oliveira Santos +6 more