Results 1 to 10 of about 2,553,530 (166)
Effects of Ce, Sm and Yb on cavitation erosion of NAB alloy in 3.5% NaCl solution
The influences of Ce, Sm and Yb on cavitation erosion of NAB alloy in 3.5% NaCl solution are evaluated using mass loss, SEM, 3D morphology and Tafel plot, respectively. The results show that the addition of Ce or Sm or Yb enhances the mechanical property
D.G. Li, S.L. Song, D.R. Chen, P. Liang
doaj +1 more source
Two kinds of Ti-alloys, i.e., Al–5Ti and Al–10Ti alloys, were manufactured in this study, and their ultrasonic cavitation erosion behaviors in 3.5 wt.% NaCl solution were evaluated by the cumulative mass loss, scanning electronic micrograph, and three ...
Jingtao Zhao +3 more
doaj +1 more source
Al and Al-5Ti alloys were manufactured by an ultrasonic casting method with a new device, and their ultrasonic cavitation erosion behaviors of Al and Al-5Ti alloys in the distilled water were clarified.
Jingtao Zhao +4 more
doaj +1 more source
The cavitation erosion behavior of Fe-based amorphous/nanocrystalline coatings has been investigated in specimens prepared by arc spraying process. The cavitation erosion test was performed in a vibratory cavitation apparatus using 3.5 wt% NaCl solution.
Jinran Lin +5 more
doaj +1 more source
Laser cavitation is a novel surface modification technology using the impact of bubble collapse and laser-induced plasma to induce plastic deformation and produce compressive residual stress on material surfaces.
Chunhui Luo, Jiayang Gu
doaj +1 more source
Different from additive manufacturing and subtractive manufacturing, iso-material manufacturing (also named isovolumetric manufacturing) is applied to 304 stainless steel (304SS) by laser surface melting (LSM) at four energy density (51 J/mm2, 44 J/mm2 ...
B.S. Cao +5 more
doaj +1 more source
Effect of Ultrasonic Shot Peening on the Cavitation Erosion Resistance of SLM316L Stainless Steel [PDF]
In order to investigate the effect of ultrasonic shot peening on the cavitation erosion resistance of SLM316L stainless steel, the surface of SLM316L stainless steel was treated for varying durations (5, 25 and 45 min) using an ultrasonic shot peening ...
WANG Zenan, CHENG Feng, WANG Shuo, SUN Jie
doaj +1 more source
In this article, the WC-10Ni coatings were fabricated by HVOF spray, then the ultrasonic cavitation erosion performances of the coatings in distilled water and 3.5 wt% NaCl solution with various Na2S concentrations (0, 20 and 200 ppm) were investigated ...
Ziyu Wei +4 more
doaj +1 more source
CoCrxFeMnNi (x represents the atomic percentage of Cr element, x = 20, 25, 30, and 35, denoted as Cr20, Cr25, Cr30, and Cr35 alloys) high-entropy alloy (HEA) coatings were cladded by plasma arc on the surface of 0Cr13Ni5Mo steel.
Kaige Zhang +6 more
doaj +1 more source
Cavitation erosion is one of the key reasons for the failure of hydraulic machinery, ship propellers, valves and other flow-through components, seriously affecting the operational efficiency and service life of equipment.
Hongbin Lin +5 more
doaj +1 more source