Results 11 to 20 of about 266 (165)
Peening Natural Aging of Aluminum Alloy by Ultra-High-Temperature and High-Pressure Cavitation
The peening solution treatment was performed on AC4CH aluminum alloy by ultra-high-temperature and high-pressure cavitation (UTPC) processing, and the peening natural aging was examined.
Toshihiko Yoshimura +2 more
exaly +3 more sources
Suppression of Fatigue Crack Propagation of Duralumin by Cavitation Peening
It was demonstrated in the present paper that cavitation peening which is one of the mechanical surface modification technique can suppress fatigue crack propagation in duralumin.
Hitoshi Soyama +3 more
doaj +2 more sources
Numerical and Experimental Studies of Cavitation Behavior in Water-Jet Cavitation Peening Processing [PDF]
Water-jet cavitation peening (WCP) is a new technology for the surface modification of metallic materials. The cavitation behavior in this process involves complex and changeable physics phenomena, such as high speed, high pressure, multiple phases ...
H. Zhang, B. Han, X.G. Yu, D.Y. Ju
doaj +2 more sources
Effect of Cavitation Peening on Fatigue Properties in Friction Stir Welded Aluminum Alloy AA5754
Friction stir welding (FSW) is an attractive solid-state joining technique for lightweight metals; however, fatigue properties of FSWed metals are lower than those of bulk metals.
Hitoshi Soyama +2 more
doaj +1 more source
The current work investigates the erosion‐corrosion behaviour of thermally sprayed tungsten carbide‐10% nickel (WC‐10% Ni) coatings placed on the AA6061 aluminum alloy. The AA6061 aluminum alloy was coated with tungsten carbide –10% nickel coatings utilising a high‐velocityoxy‐fuel (HVOF) spray method.
G. S. Pradeep Kumar +7 more
wiley +1 more source
Application of Hilbert instantaneous spectrum on improved bolt anchoring quality detection
A method utilizing a way to compute the instantaneous frequency curve of the bolt signal is proposed to overcome the phase folding problem existing in the Hilbert transform spectrum. The instantaneous frequency curve of the signal can help accurately identify the reflected signal from the bolt bottom and the position of the defect, thus accurately ...
Chen Li, Guozhong Gao, Yunsheng Wang
wiley +1 more source
Shot peening and physical vapor deposition (PVD) coatings provide increased wear resistance to tools of high‐speed steel (HSS). However, high heat input of coating processes leads to the relaxation of previously induced compressive residual stresses and strain‐hardening.
Kirsten Bobzin +5 more
wiley +1 more source
Abstract Understanding the mechanisms and controlling the possibilities of surface nanostructuring is of crucial interest for both fundamental science and application perspectives. Here, we report a direct experimental observation of laser‐induced periodic surface structures (LIPSS) formed near a predesigned gold step edge following single‐pulse ...
Pavel N. Terekhin +8 more
wiley +1 more source
Inner surface peening for long and narrow helical pipe using acoustic cavitation
The inner surface peening of helical pipes is highly challenging due to the inaccessibility of the inner surface. To the end, we propose to peen the inner surface by introducing acoustic cavitation inside the pipe. We also provide a theory to account for
Prabhu Murugesan +2 more
doaj +1 more source
The submerged high‐pressure water jet has the characteristics of high velocity, strong turbulence, and severe cavitation. In order to reveal the formation mechanism of shear cavitation in the submerged high‐pressure water jet and to grasp the turbulent structure and velocity distribution characteristics in the jet, the prediction ability of different ...
Yongfei Yang +6 more
wiley +1 more source