Results 201 to 210 of about 47,956 (293)
Hydrochar‐mill‐scale briquettes with varying C/O molar ratios (0.07–0.90) have been tested at 1650 °C to evaluate their slag foaming performance for electric arc furnace application. All seven briquette recipes developed succeed in promoting slag foaming.
Yu‐Chiao Lu +3 more
wiley +1 more source
H2 prereduction selectively metallizes Fe in UG2 chromite pellets at 1100°C, while silicon carbide becomes active at 1300°C to convert remaining Cr2O3 to carbides and promote Cr metallization. By separating the roles of H2 and SiC, the sequential route reaches up to 65.7% Cr metallization and suppresses in‐furnace CO generation by ≈75% versus ...
D. Coertzen +5 more
wiley +1 more source
Conversion of a Polyolefin Mixture into Light Olefins by Fast Pyrolysis and In-Line Catalytic Cracking on HZSM‑5. [PDF]
Ciccone B +7 more
europepmc +1 more source
This study investigates the reduction behavior of two international iron ores, including a synthetic hematite produced by oxidation of magnetite, in a novel fluidized‐bed kinetic reactor at elevated pressures. The reduction takes place at various temperatures (650°C, 700°C, and 750°C), and various hydrogen partial pressures (30, 55, and 80 vol% H2 ...
Valentina Nigitz +5 more
wiley +1 more source
Hard Carbon Anodes for Sodium-Ion Batteries: Industrial Precursors, Structural Regulation, and Future Prospects. [PDF]
Yang L +10 more
europepmc +1 more source
Commercial iron ore sinter is reduced isothermally under operation‐derived radial blast furnace gas atmospheres with and without 20 kg H2/tHM injection. Hydrogen improves reduction at 900–1100 °C, whereas at 700 °C the high H2O content limits the wüstite‐to‐iron driving force.
Ahmed Abdelrahim +5 more
wiley +1 more source
Unveiling the role of local temperature gradients in individual zeolites containing metal active sites. [PDF]
Zhao B +10 more
europepmc +1 more source
Biocarbon injection is investigated as a promising pathway for sustainable electric arc furnace steelmaking using a combined experimental–numerical approach. Results demonstrate that biocarbon can effectively penetrate slag and generate intense foaming within a defined operating window.
Christopher DiGiovanni +6 more
wiley +1 more source
Unveiling the Catalytic Pyrolysis Behavior and Kinetics of Epoxy Resin over Niobium Oxide-Tailored ZSM‑5 Zeolites. [PDF]
Pan S +8 more
europepmc +1 more source
In primary electric arc furnace (EAF) steelmaking, carbon boiling removes nitrogen from liquid steel and sustains slag foaming. In 100% scrap‐ or hydrogen direct reduced iron (HDRI)‐based EAF steelmaking, carbon boiling is absent; therefore, carbonaceous material and oxygen injection into the slag is needed to maintain foaming and avoid nitrogen ...
Zushu Li +3 more
wiley +1 more source