Results 21 to 30 of about 18,762 (268)
The Use of APS Thermal Barrier Coatings in Corrosive Environments [PDF]
Thermal barrier coatings (TBC) can be used to reduce the metal temperature of gas turbine blades enabling higher Cr alloys (lower strength) to be used when gas turbines are to be used in corrosive environments (where hot corrosion resistance is required).
Wells, Jonathan +3 more
openaire +3 more sources
The inhibition effect of four inhibitors of sodium citrate (SC), sodium dodecylbenzenesulphonate (SDBS), diammonium phosphate ((NH4)2HPO4) and sodium vanadate (NaVO3) on the corrosion behaviour of AM60 magnesium alloy in 0.1 M sodium chloride (NaCl ...
Dan Liu +3 more
doaj +1 more source
Sweet Corrosion Inhibition by CO2 Capture
The most practical and economical way to combat the problems derived from CO2 corrosion (sweet corrosion) is the use of corrosion inhibitors of organic origin.
Jesus Porcayo-Calderon +3 more
doaj +1 more source
High Temperature Water Oxygen Corrosion Mechanism of Ytterbium Disilicate Environmental Barrier Coatings [PDF]
The composite components of ceramic matrix face serious water oxygen corrosion degradation in the aeroengine gas environment. The application of environmental barrier coatings on the surface of components for thermal protection is an effective measure to
HU Xiangpeng, JIANG Wenhao, LI Biao
doaj +1 more source
This paper studied corrosion of pure Mg and the Mg alloys EV31A, WE43B, ZE41A, coated with commercial corrosion inhibiting compounds (CICs) (LPS 3, LPS2, AMLGuard, Ardrox 3961) immersed in 3.5 wt% (0.6 M) NaCl solution saturated with Mg(OH)2.
Akif Soltan +6 more
doaj +1 more source
Secondary corrosion barriers: Application [PDF]
A program to develop a new fuel element was initiated at Hanford in 1951. A survey of the possible methods of making such a fuel element was completed and a document listing all possible lines of research was written. The problem was outlined as it appeared at that time; various developments which have occurred subsequently have changed this problem to
openaire +2 more sources
General Corrosion and Localized Corrosion of Waste Package Outer Barrier [PDF]
The waste package design for the License Application is a double-wall waste package underneath a protective drip shield (BSC 2004 [DIRS 168489]; BSC 2004 [DIRS 169480]). The purpose and scope of this model report is to document models for general and localized corrosion of the waste package outer barrier (WPOB) to be used in evaluating waste package ...
openaire +2 more sources
Corrosion behavior of hot-dipped zinc-based coatings (pure zinc, Zn–0.25%Al and Zn–5%Al) was studied through potentiodynamic polarization test and electrochemical impedance spectroscopy in 3.5% NaCl solution.
Yang Liu, Hongying Li, Zhenguo Li
doaj +1 more source
Hot Corrosion Resistance of Thermal Barrier Coatings [PDF]
The hot corrosion resistance of yttria stabilized zirconia (YSZ) thermal barrier coatings was evaluated using an atmospheric burner rig. The coatings were deposited by plasma spraying and electron beam physical vapor deposition (EB-PVD). The tests were performed for up to 2000 hours at 1700°F and 1300°F.
B. A. Nagaraj +4 more
openaire +1 more source
Within the multi-barrier system proposed for the permanent disposal of used nuclear fuel, the primary engineered barrier is the sealed metallic container.
Thalia E. Standish +5 more
doaj +1 more source