Degradation Pathways of Silicon‐Based Anodes in Lithium‐Ion Batteries

open access: yesAdvanced Energy Materials, EarlyView.
Silicon‐based anodes undergo degradation through five primary pathways: (1) mechanical and structural deterioration of the active material, (2) loss of electrode integrity and electrical contact, (3) mechanical instability of the solid electrolyte interphase (SEI), characterized by repetitive fracture and deformation, (4) chemical instability of the ...
Yoon Jeong Choi   +3 more
wiley   +1 more source

Lattice Coherency‐Driven (111)‐Oriented Wide Bandgap Perovskite Films

open access: yesAdvanced Energy Materials, EarlyView.
Methylammonium lead chloride (MAPbCl3)‐derived seed templates regulate wide‐bandgap perovskite crystallization through coupled thermodynamic and kinetic effects. Lattice‐coherent templating lowers the energy cost for (111) epilayer growth, while growth retardation controls crystallization kinetics, ultimately producing highly crystalline face‐up (111 ...
Yu‐Na Lee   +5 more
wiley   +1 more source

AI-Based Triage Decision Support: Multisite Economic Evaluation in the United States. [PDF]

open access: yesJ Med Internet Res
Levin S   +7 more
europepmc   +1 more source

Multiscale Perspectives on Perovskite Instability: From Atomistic Deformation to Device Degradation in Perovskite Solar Cells

open access: yesAdvanced Energy Materials, EarlyView.
Multiscale perspectives on how excess charges in soft lead halide perovskites induce operational instability in photovoltaic devices are presented. Localized carriers formed under thermodynamic non‐equilibrium states modify atomistic interactions and drive lattice distortions, accelerating device degradation.
Joo‐Hong Lee   +6 more
wiley   +1 more source

A Quantitative Lithium Inventory Framework for Anode‐Free Lithium Metal Batteries

open access: yesAdvanced Energy Materials, EarlyView.
A component‐resolved lithium inventory framework quantitatively tracks Li redistribution across the cell in anode‐free NMC622||Cu pouch cells throughout cycling. Three sequential degradation stages are identified: formation‐driven cathode Li depletion, midlife inactive Li0 accumulation, and late‐stage runaway SEI thickening. The cathode, as the sole Li
Wurigumula Bao   +9 more
wiley   +1 more source

Water‐Mediated Proton Facilitation for Stable Acidic CO2 Electrocatalysis

open access: yesAdvanced Energy Materials, EarlyView.
Proton‐mitigating Cu─O─Ce sites accelerate *CO formation and PCET‐mediated *CO─*CHO coupling, enabling efficient multicarbon production at relatively low current density. Maintaining a retentive acidic pH suppresses parasitic hydrogen evolution and preserves in situ CO2 availability for carbon‐efficient acidic CO2 reduction.
Jeong Hyun Hwang   +13 more
wiley   +1 more source

Evaluating the costs of developing a digital supervision tool for task-shared depression care: findings from a multi-site study in India. [PDF]

open access: yesBJPsych Open
Kamat S   +11 more
europepmc   +1 more source

Home - About - Disclaimer - Privacy