Results 141 to 150 of about 1,661,643 (275)
Deuterium Retention in NSTX with Lithium Conditioning
High (≈ 90%) deuterium retention was observed in NSTX gas balance measurements both withand without lithiumization of the carbon plasma facing components.
C.H. Skinner, J.P. Allain, W. Blanchard, H.W. Kugel, R. Maingi, L. Roquemore, V. Soukhanovskii, C.N. Taylor
core
Comparative study of deuterium retention and vacancy content of self-ion irradiated tungsten
A. Hollingsworth +21 more
semanticscholar +1 more source
Effects of zirconium element on the microstructure and deuterium retention of W-Zr/Sc2O3 composites. [PDF]
Chen H +8 more
europepmc +1 more source
Deuterium retention in MeV ion-irradiated beryllium
A. Založnik +4 more
semanticscholar +1 more source
Differentiating the role of lithium and oxygen in retaining deuterium on lithiated graphite plasma-facing components [PDF]
Laboratory experiments have been used to investigate the fundamental interactions responsible for deuterium retention in lithiated graphite. Oxygen was found to be present and play a key role in experiments that simulated NSTX lithium conditioning, where
Taylor, C.N. +5 more
core
Carboxymethyl cellulose‐based biopolymer optical fibers are fabricated using aqueous wet spinning. The fibers exhibit record‐low optical attenuation in polysaccharide‐based waveguides while maintaining efficient transmission across the visible‐to‐near‐infrared region of the electromagnetic spectrum.
Jani Patrakka +3 more
wiley +1 more source
“Dead Lithium” Formation and Mitigation Strategies in Anode‐Free Li‐Metal Batteries
Anode‐free lithium metal batteries, though promising due to their high energy density, face challenges from dead lithium formation. “Dead lithium”, disconnected from the anode, causes capacity loss, increased resistance, and safety risks. This review explores the origins of dead lithium, its impact on battery performance, and potential strategies for ...
Mozaffar Abdollahifar, Andrea Paolella
wiley +1 more source
Deuterium desorption and retention of Beryllium intermetallic compounds for fusion applications
Beryllium intermetallic compounds (beryllides) such as Be12Ti and Be12V are the most promising advanced neutron multipliers in demonstration (DEMO) power reactors because of their low swelling and high stability at high temperatures.
944740 +15 more
core
Deuterium Retention and Surface Modification of TungstenAlloys produced by Powder Injection Moulding afterDeuterium Plasma ExposureRobert Krug1∗, Sören Möller1, Steffen Antusch2, Marcin Rasinki1,Arkadi Kreter1, Marius Wirtz1, Bernhard Unterberg11 ...
Krug, Robert +6 more
core
Aim Londamocitinib (AZD4604) is an inhaled, selective Janus kinase 1 (JAK1) inhibitor in development for asthma. This open‐label, two‐part, phase I clinical study (NCT06157255) used a radiolabelled microtracer approach to evaluate the absolute bioavailability and the absorption, distribution, metabolism and excretion (ADME) of inhaled londamocitinib ...
Camille Riff +12 more
wiley +1 more source