Results 11 to 20 of about 1,661,643 (275)
Deuterium retention in tungsten studied by sequential implantations at ELM-relevant energies
Plasma edge-localized modes (ELMs) can cause considerable fuel retention in fusion reactor vessel walls by implanting plasma particles with high energies and fluxes.
T. Vuoriheimo +6 more
doaj +2 more sources
Influence of redeposited tungsten and EUROFER97 layers on deuterium retention in plasma-facing materials [PDF]
Retention of hydrogen isotopes in plasma-facing materials is a key challenge for safety and fuel efficiency of nuclear fusion reactors. In realistic reactor environments, simultaneous processes, such as erosion, redeposition, implantation and outgassing,
Martina Fellinger +4 more
doaj +3 more sources
Deuterium retention and blistering in tungsten foils
To investigate deuterium retention and the onset of blistering, deuterium was implanted in cold rolled tungsten foils at fluences ranging from 3 ×1020 to 3 ×1022D/m2.
C.N. Taylor, M. Shimada, B.J. Merrill
doaj +2 more sources
Sputter-deposited thin films (33–1160 nm) from EUROFER97 were obtained on different substrates (C, Si, W, MgO) in argon and a mix of argon and deuterium atmosphere. The composition, microstructure, and mechanical properties of the films were analyzed and
E. Pitthan +9 more
doaj +2 more sources
Deuterium retention in silicon carbide, SiC ceramic matrix composites, and SiC coated graphite [PDF]
Silicon Carbide (SiC) is a low Z material discussed as an alternative to graphite for fusion devices. The retention of hydrogenous species is an important plasma-surface interaction property.
Markus T. Koller +7 more
doaj +2 more sources
Hydrogen permeation and retention in deuterium plasma exposed 316L ITER steel
Fuel permeation and retention in fusion reactor wall materials are important issues for plasma operation and safety reasons in ITER. The austenitic stainless steel 316L(N)-IG will be used as structural material in the first wall components in ITER.
A. Houben +5 more
doaj +2 more sources
EUROFER97 steel samples were exposed to deuterium plasma in the linear plasma device PISCES-A with the ion energies of 90 and 140 eV at exposure temperatures between 360 and 773 K to deuterium ion fluences between 3.8 × 1023 and 6.3 × 1025 m−2.
V.Kh. Alimov +5 more
doaj +2 more sources
Effect of microstructure and neutron irradiation defects on deuterium retention in SiC [PDF]
Retention of hydrogen isotopes is a critical concern for operating fusion reactors as retained tritium both activates components and removes scarce fuel from the fuel cycle.
Alex Leide +6 more
doaj +3 more sources
Tungsten targets were first irradiated with high energy W6+ ions (20 MeV) with different dose rates at 800 K and then loaded with deuterium at room temperature to decorate the displacement damage created in the first step.
Thomas Schwarz-Selinger +2 more
exaly +2 more sources
Deuterium Retention in Tungsten Simultaneously Damaged by High Energy W Ions and Loaded by D Atoms
Deuterium retention was for the first time measured in tungsten samples simultaneously irradiated by W ions and exposed to D atoms at five different temperatures from 450K to 1000K. In order to obtain information on the defect concentration, samples were
Thomas Schwarz-Selinger +2 more
exaly +3 more sources