Results 81 to 90 of about 6,850 (263)

Metal Battery Anode: Rich in Electrons, Rich in Problems: A Critical Review from Industrial Perspectives

open access: yesAdvanced Science, EarlyView.
Metal‐anode batteries using Li, Na, Mg, and Ca offer exceptionally high energy density, but dendrites, unstable interphases, cracking, and pore formation hinder durability and safety. This review shows how careful electrolyte and interphase design can stabilize these reactive metals.
Jian Pan   +3 more
wiley   +1 more source

Ductile B2 Intermetallics‐Driven Strength‐Ductility Synergy in Heterolaminated Multi‐Principal Element Alloys

open access: yesAdvanced Science, EarlyView.
Intrinsic phase toughening transforms a brittle B2 intermetallic into a plastically deformable, load‐bearing phase, while a heterogeneous laminated architecture suppresses strain localization and interface cracking. The synergy between ductile intermetallics and mesoscale heterogeneity establishes a general design strategy for breaking the long ...
Lu Yang   +9 more
wiley   +1 more source

Surface and Interfacial Engineering toward Durable Mechanically Coupled Flexible Electronics

open access: yesAdvanced Science, EarlyView.
This Review highlights how surface and interfacial engineering governs the reliability, durability, and functional stability of mechanically coupled flexible electronics. By integrating fundamental interfacial theory, failure mechanisms, multiscale engineering strategies, and representative applications, it provides a design‐oriented framework for ...
Qian Wang, Fangfang Dai, Wei Wu
wiley   +1 more source

Low Temperature Impact Toughness of Steel S355NL for Wind Power Tower Flange

open access: yesTeshugang, 2015
The tangential and axial impact toughness of steel S355NL for wind power tower flange (/% : 0.14C, 0.22Si, 1.35Mn, 0.010P, 0.002S, 0.06Cr, 0.01Mo, 0.l0Ni, 0.03Cu, 0.40Ceq) at -20~-80℃ has been tested and analyzed.
戈文英
doaj  

The influence of sliding velocity and temperature on the ductile-to-brittle transition in asperity-level wear: A molecular dynamics study

open access: yesFriction
During sliding contact, asperities may undergo either ductile smoothing or brittle fracture, producing debris. A critical junction scale, d∗, governed by material properties, dictates this transition.
Sacha Zenon Wattel   +1 more
doaj   +1 more source

Self‐Assembly of Organic–Inorganic Copolymers Toward Bio‐Inspired Cementitious Composites

open access: yesAdvanced Science, EarlyView.
Organic–inorganic copolymerization of calcium silicate hydrate and thioctic acid produces a self‐organized nanocomposite inspired by the disordered collagen–mineral architecture of trabecular bone. The resulting material combines a compressive strength above 300 MPa with intrinsic physical reprocessibility, retaining over 80% of its strength and energy
Zonglin Xie   +8 more
wiley   +1 more source

Fracture Toughness Testing in the Ductile-Brittle Transition Region

open access: yes, 1989
Fracture toughness testing in the ductile-brittle transition regime is often problematic. In this region both constraint effects as well as ductile tearing will affect the brittle fracture probability. This causes the scatter to grow very large in the transition region.
openaire   +3 more sources

Bio‐Based Polyurethanes for Sustainable and Multifunctional Applications

open access: yesAdvanced Science, EarlyView.
Bio‐based polyurethanes prepared from vegetable oils, lignin, and polysaccharides have attracted increasing interest as alternatives to fossil‐derived polyurethanes. This review summarizes recent progress in their chemistry, structural engineering, and advanced applications, highlighting the roles of feedstocks, chain‐segment design, dynamic covalent ...
Xin Li   +6 more
wiley   +1 more source

Stress modeling for the upper and lower crust along the Anninghe, Xianshuihe, and Longmenshan Faults in southeastern Tibetan plateau

open access: yesFrontiers in Earth Science
Earthquake occurrence depth in the crust is related to stress, temperature, and brittle–ductile transition, which is also near the transition depth of the upper to lower crust. The composition variation between the upper and lower crust causes remarkable
Junshan Xu, Xiangfang Zeng
doaj   +1 more source

Intrinsic Mechanical Parameters and their Characterization in Solid‐State Lithium Batteries

open access: yesAdvanced Energy Materials, Volume 15, Issue 11, March 18, 2025.
This review focuses on the intrinsic mechanical parameters and their associated characterization in solid‐state batteries. The physical significance of mechanics parameters is introduced with exhaustive classifications by elastic, plastic deformations and fracture in bulk, adhesion, friction at interfaces, and mechanical fatigue in cells ...
Shuai Hao   +5 more
wiley   +1 more source