Results 51 to 60 of about 3,681,759 (294)
Two-stage preheating is used in selective electron beam melting (SEBM) to prevent powder spreading during additive manufacturing (AM); however, its effects on part properties have not been widely investigated.
Chu Lun Alex Leung +5 more
doaj +1 more source
Summary: The structure of lithium (Li) metal anode, including the Li metal and the solid electrolyte interphase (SEI), is critical to the investigation of cycle stability or decay mechanisms.
Xiangyan Li +9 more
doaj +1 more source
Experiments and thermophysical simulations were conducted to investigate the electron beam powder bed fusion electron beam (PBF‐EB/M) process for the γ′‐strengthened nickel‐based superalloy Inconel 738LC. The results demonstrate the impact of process‐induced microstructural variations on high‐temperature mechanical behavior, providing a basis for ...
Jan Niklas Petenati +11 more
wiley +1 more source
Prediction of coronary events with electron beam computed tomography
We sought to determine the prognostic accuracy of electron beam computed tomographic (EBCT) scanning of the coronary arteries at three to four years.Coronary artery calcium scores determined by EBCT correlate with the severity of coronary artery disease.
Arad, Yadon +4 more
openaire +2 more sources
Porous γ-TiAl Structures Fabricated by Electron Beam Melting Process
Porous metal structures have many benefits over fully dense structures for use in bio-implants. The designs of porous structures can be made more sophisticated by altering their pore volume and strut orientation. Porous structures made from biocompatible
Ashfaq Mohammad +5 more
doaj +1 more source
Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi +5 more
wiley +1 more source
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas
wiley +1 more source
APT mass spectrometry and SEM data for CdTe solar cells
Atom probe tomography (APT) data acquired from a CAMECA LEAP 4000 XHR for the CdS/CdTe interface for a non-CdCl2 treated CdTe solar cell as well as the mass spectrum of an APT data set including a GB in a CdCl2-treated CdTe solar cell are presented ...
Jonathan D. Poplawsky +5 more
doaj +1 more source
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt +5 more
wiley +1 more source
This article investigates the dependence of the properties on the manufacturing orientation in the form of the inclination angle to the build plate of LPBF‐fabricated NiTi rods with a diameter of 150–220 µm. Metallographic, chemical, thermal, and mechanical characterization show behavior under identical manufacturing conditions that ranges from ...
Sandra Herzig +2 more
wiley +1 more source