Results 201 to 210 of about 156,071 (279)
Residual adhesive after electrode loading in adhesive‐assisted resistance spot welding is quantified through a traceable experimental‐to‐digital workflow. Chromatic confocal topography provides calibrated surface‐height data, while OpenCV detects the electrode imprint and integrates adhesive height into comparable volume metrics.
Sung‐Min Wi, Jiangdong Zhao
wiley +1 more source
Electrical Property Enhancement of a Breast-Fat-Equivalent Phantom for Microwave Mammography. [PDF]
Inada K, Nozaki Y, Yamamoto T.
europepmc +1 more source
We apply a foundational machine‐learning interatomic potential based on the graph atomic cluster expansion (GRACE) to simulate the commercial Ni‐based single‐crystal superalloy CMSX‐4. Hybrid Monte‐Carlo/molecular dynamics sampling resolves short‐range order in the γ phase and L12 sublattice occupancies in the γ’ phase and connects them to stacking ...
Aditya Vishwakarma +4 more
wiley +1 more source
Femoral finite element analysis of a novel cementless revision total knee arthroplasty system. [PDF]
Dong Z +7 more
europepmc +1 more source
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt +5 more
wiley +1 more source
Contactless Microwave-Based Estimation of Complex Permittivity of Masonry Materials: A Frequency-Domain Approach. [PDF]
Szczepaniak Z +4 more
europepmc +1 more source
Deep‐UV (258 nm) femtosecond pulses enable uniform amorphous silicon writing on Si(100)/(111) with a six‐fold larger fluence amorphization window than NIR methods. Optimized fluence and overlap yield 20–45 nm uniform and continuous amorphous layers. Microscopy shows sharp interfaces, and real‐time reflectivity reveals nanosecond melt–resolidification ...
Wissal Benali +5 more
wiley +1 more source
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...
Sameh Dabees +6 more
wiley +1 more source