Results 41 to 50 of about 10,603 (221)

Low-Temperature Impact Fracture Behavior of Medium Manganese Steel with Bcc-fcc Duplex Microstructures

open access: yesMetals
Impact fracture behavior at low temperatures was investigated in medium manganese steel with bcc-fcc duplex microstructures. The impact energy was above 150 J (−80~20 °C) and the fractography showed dimples for inter-critical annealing at 630 °C (QHA ...
Yu Du   +6 more
doaj   +1 more source

Effects of hydrogen gas pressure and test frequency on fatigue crack growth properties of low carbon steel in 0.1-90 MPa hydrogen gas

open access: yesNihon Kikai Gakkai ronbunshu, 2014
In order to investigate the effects of hydrogen gas pressure pH2 and test frequency f on the fatigue crack growth (FCG) properties of low carbon steel in hydrogen gas atmosphere, the FCG tests using compact tension specimens were conducted under various ...
Michio YOSHIKAWA   +4 more
doaj   +1 more source

Off-Axis Tension Behaviour of Unidirectional PEEK/AS4 Thermoplastic Composites

open access: yesApplied Sciences, 2023
An experimental method for non-standard off-axis tension tests of unidirectional composites is developed. A new oblique end-tab is designed to eliminate stress concentration and in-plane bending moment induced by off-axis tension loading.
Yifan Ma, Yazhi Li, Lu Liu
doaj   +1 more source

Fatigue Behavior of an Al-12.7Si-0.7Mg Alloy Processed by Extrusion and Heat Treatment

open access: yesFrontiers in Materials, 2021
The fatigue life of a hot extruded Al-12.7Si-0.7Mg alloy under T1, T4, and T6 conditions was studied. The microstructure and tensile properties of the alloy were investigated in order to analyze the fatigue behavior.
Fang Liu, Fuxiao Yu, Dazhi Zhao, Li Gao
doaj   +1 more source

Effect of Hydrogen Content and Strain Rate on Hydrogen-induced Delay Cracking for Hot-stamped Steel

open access: yesMetals, 2019
Hot-stamped steel has been widely used in automobile bumper and other safety components due to its high strength. Therefore, this paper investigates the effect of hydrogen content and strain rate on hydrogen-induced delay cracking (HIDC) behavior.
Hongxing Jia   +4 more
doaj   +1 more source

The Combined Effect of Banana Fiber and Fly Ash Reinforcements on the Mechanical Behavior of Polyester Composites

open access: yesJournal of Natural Fibers, 2022
The mechanical behavior of banana fiber (BA) reinforced polymer composites filled with fly ash (FA) is analyzed in this present investigation. Polyester matrix is used to produce composites with 30% of banana fiber volume and fly ash with three separate ...
Gokul Kannan   +3 more
doaj   +1 more source

Integrity Assessment of Stress Corrosion Cracking Susceptibility of Duplex UNS S32205 and Austenitic UNS S31653 Stainless Steel Reinforcements

open access: yesMetals, 2023
Herein, the stress corrosion cracking (SCC) susceptibility of duplex (UNS S32205) and austenitic (UNS S31653) stainless steel (SS) reinforcements was evaluated using integrity assessment criteria.
Ulises Martin, David M. Bastidas
doaj   +1 more source

Fracture morphology of carbon fiber reinforced plastic composite laminates

open access: yesMaterials Research, 2010
Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications.
Vinod Srinivasa   +6 more
doaj   +1 more source

Experimental investigation of shape memory polymer hybrid nanocomposites modified by carbon fiber reinforced multi-walled carbon nanotube (MWCNT)

open access: yesMaterials Research Express, 2021
This paper presents the effect of the variations of multi-walled carbon nanotube (MWCNT) modification in shape memory polymer hybrid composites concerning their mechanical, thermomechanical, and shape memory characterizations.
Kanif Markad, Achchhe Lal
doaj   +1 more source

Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales

open access: yesAdvanced Engineering Materials, EarlyView.
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik   +7 more
wiley   +1 more source