Results 21 to 30 of about 8,376 (173)
Herein, the stress corrosion cracking (SCC) susceptibility of duplex (UNS S32205) and austenitic (UNS S31653) stainless steel (SS) reinforcements was evaluated using integrity assessment criteria.
Ulises Martin, David M. Bastidas
doaj +1 more source
Fractographic Analysis Of Selected Boron Steels Subjected To Impact Testing
In this paper dynamic properties of low-alloy boron steels – Hardox 500, B27 and HTK 900H in delivered state (after hardening and tempering) are considered.
Dudziński W. +2 more
doaj +1 more source
Fractography of Bone Using Reconstructed Computed Tomography (CT) Scans: A Case Report Series
Fractography has been shown to be applicable to forensic assessments of skeletal trauma by observing the presence and orientation of fracture surface features, which reveal information about the direction of crack propagation.
Decker, Summer, Christensen, Angi
core +1 more source
The effect of microstructure on impact properties of AH80DBD low carbon bainite steel is analyzed by macro-fractography, scanning fractography, metallography and transmission electron microscope.
陈尹泽, 李娜, 宋立伟, 马志强
doaj
Light and electron microscopy of microstructure and fractography of an ultrahigh-strength martensitic steel [PDF]
Microstructure, tensile properties and fractography have been examined in the oil-quenched samples of a low-alloy ultrahigh strength 4340 steel. Intergranular fracture was revealed to locate at the fracture origin.
Wang, Wei +6 more
core +4 more sources
The effect of platinum-aluminide coating features on high-temperature fatigue life of nickel-based superalloy Rene®80 [PDF]
Low cycle fatigue is the most important failure mode in Aviation/Industrial engine rotary turbine parts. In this paper, the influence of Pt-aluminide coating parameters on high temperature low cycle fatigue behavior of superalloy Rene®80 which is used to
Barjesteh M.M. +3 more
doaj +1 more source
Impact fracture behavior at low temperatures was investigated in medium manganese steel with bcc-fcc duplex microstructures. The impact energy was above 150 J (−80~20 °C) and the fractography showed dimples for inter-critical annealing at 630 °C (QHA ...
Yu Du +6 more
doaj +1 more source
Effect of Hydrogen Content and Strain Rate on Hydrogen-induced Delay Cracking for Hot-stamped Steel
Hot-stamped steel has been widely used in automobile bumper and other safety components due to its high strength. Therefore, this paper investigates the effect of hydrogen content and strain rate on hydrogen-induced delay cracking (HIDC) behavior.
Hongxing Jia +4 more
doaj +1 more source
Effect of Dialkyl Peroxide Blending on Tensile Properties of PLA/PBAT Polymer Alloys
Poly(lactic acid) (PLA) and poly(butylene adipate/terephthalate) (PBAT) were used for polymer alloys, and the effects of the mixing ratio of PLA and PBAT and the addition of dialkyl peroxide (compatibilizing agent) were examined. The stress-strain curves
Masahiro NISHIDA +4 more
doaj +1 more source
The mechanical behavior of banana fiber (BA) reinforced polymer composites filled with fly ash (FA) is analyzed in this present investigation. Polyester matrix is used to produce composites with 30% of banana fiber volume and fly ash with three separate ...
Gokul Kannan +3 more
doaj +1 more source