Results 61 to 70 of about 8,376 (173)
Some studies on the influence of stress ratio and test temperature on X-ray fractography observations in C45 steel specimens [PDF]
This paper deals with additional ¿X-ray fractography¿ observations made on C45 steel, subsequent to the earlier work [K. Rajanna, B. Pathiraj and B. H. Kolster, Fatigue fracture surface analysis in C45 steel specimens using X-ray fractography.
K. Rajanna +5 more
core +1 more source
The utilization of fractography to determine crack origins as well as the mechanisms of crack propagation is an established method in failure analysis.
Lüthi, Thomas (author) +2 more
core +1 more source
Tufting‐Based Manufacturing Method for High‐Performance 3D Composite Lap Joints
Graphical abstract illustrating the manufacturing process of a tufted non‐crimp preform lap joint, fractographic characterisation and comparative mechanical performance evaluation. ABSTRACT This study presents a tufting‐enabled through‐thickness reinforcement approach for enhancing the performance of 3D composite lap joints manufactured using resin ...
J. Ahmed +3 more
wiley +1 more source
Whole‐tire reclaimed rubber is upgraded with wood sawdust, a carpentry by‐product available at no cost, across loadings from 0 to 20 wt%. At 5 wt%, tensile strength, elongation, hardness, viscosity, and water absorption all stay within commercial specification, and real factory data show an annual production saving near $62,000 with no capital ...
Mohammed S. Matar +3 more
wiley +1 more source
BSA addition to physiological solutions enhances resistance of a Zn alloy to stress corrosion cracking (SCC) but reduces its corrosion resistance. Extended surface characterization explains the contrasting influences on corrosion and SCC. Unexpectedly, the alloy suffers transgranular SCC (TGSCC), despite extensive grain boundary precipitation. Thorough
RK Singh Raman +9 more
wiley +1 more source
Different molding sands generates different surface finish on casting irons. The effect of skin roughness on failure mechanism and on fatigue properties is presented in this report.
Shinde, Omkar, Omkar Shinde
core +1 more source
Investigating iodine-induced stress corrosion cracking of zirconium alloys using quantitative fractography [PDF]
Pellet Cladding Interaction (PCI) is a fuel failure phenomenon that limits power manoeuvrability of light water nuclear reactors with Iodine-Stress Corrosion Cracking (I-SCC) the most commonly hypothesised cause.
Frankel, Philipp; id_orcid +7 more
core +1 more source
To address functionality limitations in plant‐based and industrially compostable polymer aerogels, this work introduces bio‐inspired aerogels with broadened functionality. Inspired by functional plant tissues, lightweight biopolymer aerogels based on exclusively stereocomplex crystals are fabricated, featuring hierarchically macro‐/meso‐porous ...
Anthony V. Tuccitto +10 more
wiley +1 more source
An insight of the dominant fracture mechanisms occurring in mechanical metallic components during industrial service conditions is offered through this short overview.
George A. Pantazopoulos
doaj +1 more source
Overview of the study evaluating the impact of post‐print annealing on the microstructural crystallization and thermomechanical properties of FDM‐printed high‐temperature PLA and glass fiber‐reinforced PLA composites. ABSTRACT Polylactic acid (PLA) combines renewable sourcing and reliable printability with limited stiffness retention near its glass ...
Huseyin Erdem Yalkin, Ayse Nur Ozkan
wiley +1 more source