Results 111 to 120 of about 7,770 (217)

Textural fractography of fatigue failures under variable cycle loading

open access: yes, 2005
A new concept of counting time at fatigue processes is proposed, aimed to reach fractographic compatibility in cases of different loading sequences. Values of cycle effectivity are summarized to give the new reference time.
H Lauschmann (13713577)   +2 more
core  

Investigation of the Static and Dynamic Mechanical Properties of the Base Metal and Weld Zone of Haynes 25 Alloy [PDF]

open access: yesIranian Journal of Materials Science and Engineering
This work presents a comprehensive investigation of the high cycle fatigue behavior of Haynes 25 cobalt-based superalloy and its welds produced by pulsed continuous-wave (CW) laser welding.
Mahdi Behjati   +2 more
doaj  

The Fractography of Bone: Impact of Flat Bone and the Story It Tells [PDF]

open access: yes
Fractography as a method for fracture analysis has been applied widely to materials that range from glass to ceramics and polymers of varying compositions. Very limited research has been done, however, to apply this knowledge of fractography and fracture
Mendoza, Brandon   +7 more
core  

Bone Biomechanics and Fractography: Observing Trauma Characteristics in Cases from Past American Conflicts

open access: yes
This thesis explores the potential of bone fractography for use in examining skeletal trauma in burial recovery, such as in the frequent casework of the Defense Prisoner of War/Missing in Action Accounting Agency.
Cristino, Mack P.
core  

A Review of Destructive Methods for Assessing the Bulk Tensile Strength of Glass. [PDF]

open access: yesExp Mech
Damen W   +3 more
europepmc   +1 more source

Effects of Curing Schedules on Carbon-Fiber-Reinforced Laminates with a Bio-Based Epoxy Matrix. [PDF]

open access: yesPolymers (Basel)
Stroe LA   +5 more
europepmc   +1 more source

Mechanical Behavior of Conventional and Subtractively Manufactured Dental Resin Composites After Water Degradation. [PDF]

open access: yesBioengineering (Basel)
Osiceanu G   +6 more
europepmc   +1 more source