Results 181 to 190 of about 7,770 (217)
Some of the next articles are maybe not open access.
Metal Science and Heat Treatment, 2005
A brief characteristic of methods of observation, measurement, identification, and analysis of fractures is presented. Prospects of the use of the methods of fractography for solving problems of certification of materials, determining the structural mechanisms of fracture, and controlling the quality of metals are discussed.
openaire +1 more source
A brief characteristic of methods of observation, measurement, identification, and analysis of fractures is presented. Prospects of the use of the methods of fractography for solving problems of certification of materials, determining the structural mechanisms of fracture, and controlling the quality of metals are discussed.
openaire +1 more source
Abstract This article presents a brief description of the fundamental characteristics of concrete and its constituents for understanding concrete fracture surfaces. It discusses the following two types of fractures: fractures induced in the laboratory and existing (service) fractures.
openaire +1 more source
openaire +1 more source
2018
This chapter begins with a description of the different classifications of fracture, according to mechanism and extent of plastic deformation. The mechanical aspects of fracture, from the continuum mechanics and fracture mechanics points of view, are briefly described.
openaire +1 more source
This chapter begins with a description of the different classifications of fracture, according to mechanism and extent of plastic deformation. The mechanical aspects of fracture, from the continuum mechanics and fracture mechanics points of view, are briefly described.
openaire +1 more source
Quantitative Fractography for Brittle Fracture via Multilayer Perceptron Neural Network
Engineering Fracture Mechanics, 2023Lingyue Ma +2 more
exaly
2003
Abstract This article introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination and ...
openaire +1 more source
Abstract This article introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination and ...
openaire +1 more source
Abstract This article reviews the historical development of fractography, from the early studies of fracture appearance dating back to the sixteenth century, and including the development of microfractography in the middle of the 20th century, to the current state-of-the-art work in electron fractography and quantitative fractography.
openaire +1 more source
openaire +1 more source
Forensic Fractography of Bone Using Computed Tomography (CT) Scans
Journal of Forensic Radiology and Imaging, 2019Angi M Christensen, Gary M Hatch
exaly