The effect of platinum-aluminide coating features on high-temperature fatigue life of nickel-based superalloy Rene®80 [PDF]

open access: yesJournal of Mining and Metallurgy. Section B: Metallurgy, 2019
Low cycle fatigue is the most important failure mode in Aviation/Industrial engine rotary turbine parts. In this paper, the influence of Pt-aluminide coating parameters on high temperature low cycle fatigue behavior of superalloy Rene®80 which is used to
Barjesteh M.M.   +3 more
doaj   +1 more source

Erosive wear properties of ZA-27 alloy-based nanocomposites: Influence of type, amount, and size of nanoparticle reinforcements

open access: yesFriction, 2018
Metal matrix nanocomposites (MMnCs) comprise a metal matrix filled with nanosized reinforcements with physical and mechanical properties that are very different from those of the matrix.
Aleksandar Vencl   +5 more
doaj   +1 more source

Mechanical and tribological behavior of flyash, red mud and mica particles reinforced Al7075 alloy hybrid metal composites

open access: yesManufacturing Review, 2022
In the present research Al7075 alloy with 1, 3 and 5 varying weight percentages of flyash, 1, 2 and 3 varying wt.% of red mud along with constant 4 wt.% of mica particles composites were synthesized by stir casting technique.
Matti Siddesh   +5 more
doaj   +1 more source

Characterization of Corrosion and Stress Corrosion Cracking of AE44 Magnesium Alloy [PDF]

open access: yesArchives of Metallurgy and Materials, 2020
The paper presents the susceptibility of AE44 magnesium alloy to electrochemical corrosion and stress corrosion cracking (SCC). The evaluation of the intensity of the interaction of the corrosive environment was carried out using the corrosion tests and ...
M. Sozańska, A. Mościcki, B. Chmiela
doaj   +1 more source

Effect of Dialkyl Peroxide Blending on Tensile Properties of PLA/PBAT Polymer Alloys

open access: yesEngineering Transactions, 2014
Poly(lactic acid) (PLA) and poly(butylene adipate/terephthalate) (PBAT) were used for polymer alloys, and the effects of the mixing ratio of PLA and PBAT and the addition of dialkyl peroxide (compatibilizing agent) were examined. The stress-strain curves
Masahiro NISHIDA   +4 more
doaj   +1 more source

Effect of Controlled Rolling and Cooling Process on Microstructures and Mechanical Properties of Low Carbon Bainitic Steel AH80DBD

open access: yesTeshugang, 2023
The effect of microstructure on impact properties of AH80DBD low carbon bainite steel is analyzed by macro-fractography, scanning fractography, metallography and transmission electron microscope.
陈尹泽, 李娜, 宋立伟, 马志强
doaj  

Eliciting stable nanoscale fracture in single-crystal silicon

open access: yesMaterials Research Letters, 2022
In this letter, we demonstrated stable nanoscale fracture in single-crystal silicon using an in-situ wedge-loaded double cantilever beam (DCB) specimen.
Frank W. DelRio   +7 more
doaj   +1 more source

A Short Review on Fracture Mechanisms of Mechanical Components Operated under Industrial Process Conditions: Fractographic Analysis and Selected Prevention Strategies

open access: yesMetals, 2019
An insight of the dominant fracture mechanisms occurring in mechanical metallic components during industrial service conditions is offered through this short overview.
George A. Pantazopoulos
doaj   +1 more source

Fatigue Crack Growth under Non-Proportional Mixed Mode Loading in Rail and Wheel Steel Part 1: Sequential Mode I and Mode II Loading

open access: yesApplied Sciences, 2019
Fatigue tests were performed to estimate the coplanar and branch crack growth rates on rail and wheel steel under non-proportional mixed mode I/II loading cycles simulating the load on rolling contact fatigue cracks; sequential and overlapping mode I and
Makoto Akama
doaj   +1 more source

Low-Temperature Impact Fracture Behavior of Medium Manganese Steel with Bcc-fcc Duplex Microstructures

open access: yesMetals
Impact fracture behavior at low temperatures was investigated in medium manganese steel with bcc-fcc duplex microstructures. The impact energy was above 150 J (−80~20 °C) and the fractography showed dimples for inter-critical annealing at 630 °C (QHA ...
Yu Du   +6 more
doaj   +1 more source