Results 81 to 90 of about 7,291 (217)

Failure Analysis of 316L Air Cooler Stainless Steel Tube in a Natural Gas Production Field

open access: yesInternational Journal of Electrochemical Science, 2015
In spite of the excellent resistance of stainless steel (SS) towards uniform corrosion, overcoming various localized corrosion could be a real challenge. This work presents an analysis of the failure behavior of 316L SS air chiller tube with a peripheral
A. Bahgat Radwan   +4 more
doaj   +1 more source

Fractography analysis of Inconel 718 fatigued at 700°C [PDF]

open access: yes, 2016
This work deals with the fractography analysis of nickel-base superalloy Inconel 718 fatigued at 700°C in air atmosphere in the high cycle region. During cyclic loading of this alloy at high temperatures some different mechanisms compared to cyclic ...
Otakar Bokůvka   +7 more
core   +1 more source

Development of AI-Assisted Analysis Tools for the Online Fractography Database of the Fractography Working Group

open access: yes
The online fractography database of the DGM Fractography Working Group has continued to grow in recent years and currently contains more than 5,000 images of macroscopic and microscopic fracture characteristics.
I. Porohovoj, D. Bettge
core   +1 more source

Scanning Electron Microscopy Fractography Analysis of Fractured Hollow Implants

open access: yes, 2010
Fracture of the implant is one of the possible complications affecting dental implants; it is a rare event but of great clinical relevance. The aim of the present study was to perform a scanning electron microscopy (SEM) fractography evaluation of 7 ...
TRAINI T   +5 more
core   +1 more source

Application of Bone Fractography to a Medical Examiner Sample: A Case Series

open access: yes, 2018
This case study review assesses the applicability of forensic fractography of bone to forensic casework through the evaluation of four blunt-trauma cases.
Christensen, Angi M., Love, Jennifer C.
core   +1 more source

Fractography and Crack Initiation of Very-High-Cycle Fatigue for a High Carbon Low Alloy Steel

open access: yes, 2006
Very-High-Cycle Fatigue (VHCF) is the phenomenon of fatigue damage and failure of metallic materials or structures subjected to 108 cycles of fatigue loading and beyond.
钱桂安, 周承恩, 洪友士
core   +2 more sources

Synergistic effects of cold rolling and age hardening on the hardness and tensile characteristics of AA6061 hybrid composites

open access: yesMaterials Research Express
The present study involves the fabrication of aluminium alloy 6061 matrix hybrid composites with varying weight fractions of silica sand and copper particles by employing the conventional stir casting method.
Ramakrishna Vikas Sadanand   +2 more
doaj   +1 more source

Fractography and the surface crack in flexure (SCF) method for evaluating fracture toughness of ceramics

open access: yes, 1996
The surface crack in flexure (SCP) method, also known as the controlled surface flaw method, has been used to measure fracture toughness of ceramics and glasses for almost 20 years.
Kuebler, J.J. (author)   +2 more
core   +1 more source

Fractography of fatigue fractures : common features in different image textures

open access: yes, 2005
Fractography of fatigue fractures : common features in different image ...
J Sumbera (13734631)   +3 more
core  

Effect of test temperature on low-cycle fatigue of high-chromium steel with high boron and low nitrogen content

open access: yesFrontier Materials & Technologies
High-boron 9–10% chromium martensitic steels are an advanced material for manufacturing various com-ponents of thermal power units in coal-fired power plants operating under ultra-supercritical steam conditions (up to ...
Ivan S. Brazhnikov   +1 more
doaj   +1 more source