Results 91 to 100 of about 7,291 (217)
In present study, Metal Inert Gas (MIG) welding with ER309L austenitic filler wire was used to weld API X70 and SS 401 steel. This particular joint is mainly used in oil and gas plants where stainless steel need to be connected to the high strength low ...
Lochan Sharma +6 more
doaj +1 more source
This study investigates hydrogen-assisted fatigue crack growth (FCG) in vintage pipeline steels to quantify grade-dependent degradation under hydrogen–natural gas blending conditions.
Nayem Ahmed +3 more
doaj +1 more source
The investigation of structure and properties in the intermetallic compound Ni3Al, synthesized via self-propagating high-temperature synthesis (SHS-compaction) under quasi-volumetric thermal-explosion conditions, is presented in this study. The effect of
Kirill O. Akimov +2 more
doaj +1 more source
Gigacycle fatigue fractography of high Cr alloyed cold work tool steel
Betzwar-Kotas, Agnieszka +4 more
core +4 more sources
Microstructural changes and tensile fractography of Al-6061 after solutionizing and aging
This study investigates the effect of two-step heat treatment on the microstructure, mechanical properties, and fracture behavior of Al6061 alloy. Four conditions were examined: as-received and three heat-treated samples subjected to solution heat ...
Saurabh Dewangan +1 more
doaj +1 more source
Use of the helium ion microscope in small crack fractography
Highly stressed aerospace structures, such as the wing attachment points and load carry-through bulkheads of fighter aircraft, often grow fatigue cracks from micro-scale discontinuities.
Jie Tian (20496) +3 more
core
Investigation of the Static and Dynamic Mechanical Properties of the Base Metal and Weld Zone of Haynes 25 Alloy [PDF]
This work presents a comprehensive investigation of the high cycle fatigue behavior of Haynes 25 cobalt-based superalloy and its welds produced by pulsed continuous-wave (CW) laser welding.
Mahdi Behjati +2 more
doaj
Pre-stressed advanced fibre reinforced composites fabrication and mechanical performance [PDF]
Advanced composite materials have high strength-to-weight ratios, corrosion resistance and durability and are extensively used in aerospace, energy and defence industries. This research concentrates on minimising the process-induced residual stresses,
Krishnamurthy, S.
core
Mechanical characteristics and failure analysis of AA6082/TiC/graphene hybrid composites
The main aim of the present research is to improve the tensile strength of lightweight aluminium alloy 6082, which makes it fit for many advanced engineering applications.
Sohan Lal +4 more
doaj +1 more source