Results 81 to 90 of about 15,584 (255)

Crack Process Investigation in Gears Under Single Tooth Bending Fatigue Condition Using Infrared Thermography and 3D XFEM Numerical Models

open access: yesFatigue &Fracture of Engineering Materials &Structures, EarlyView.
ABSTRACT The present study proposes a combined approach of infrared thermography and 3D XFEM numerical models for crack process investigation in mechanical components such as gears. Over the years, fatigue crack analysis based on energy dissipations in the form of heat generated during fatigue tests has been widely reported, although mainly limited to ...
Luca Corsaro   +3 more
wiley   +1 more source

Fractographic Analysis Of Selected Boron Steels Subjected To Impact Testing

open access: yesArchives of Metallurgy and Materials, 2015
In this paper dynamic properties of low-alloy boron steels – Hardox 500, B27 and HTK 900H in delivered state (after hardening and tempering) are considered.
Dudziński W.   +2 more
doaj   +1 more source

Experimental Study on the Fatigue Behavior of Ti‐6Al‐4 V Bolted Joints Containing Burrs

open access: yesFatigue &Fracture of Engineering Materials &Structures, EarlyView.
ABSTRACT One‐way assembly accelerates aerospace manufacturing operations but risks leaving drilling burrs within mechanical joints. The detrimental impact of burrs on fatigue strength is widely recognized in the literature, but the mechanisms driving this “knock‐down” remain unclear. This investigation focused on mechanically fastened Ti‐6Al‐4 V single‐
Santiago Frutos Taravillo   +6 more
wiley   +1 more source

Effect of substructure fabrication method and design on the fracture resistance properties of metal–ceramic restorations

open access: yesJournal of Prosthodontics, EarlyView.
Abstract Purpose In metal–ceramic restorations, the substructure fabrication method and design may affect the prognosis of the prosthesis. This study evaluated and compared the fracture resistance of metal–ceramic restorations fabricated with different substructure fabrication methods using two different alloy powders and designs.
Young‐Hoon Lee   +4 more
wiley   +1 more source

Impact and Compressive Performance of 3D‐Printed PA6/Functionalized Graphene Nanoplatelet Sandwich Structures With Auxetic Cores

open access: yesPolymer Composites, Volume 47, Issue 18, Page 16425-16441, 20 September 2026.
Schematic of PA6/functionalized graphene nanoplatelet compounding and filament extrusion to 3D printing, sandwich panel fabrication, and mechanical characterization. ABSTRACT This study examines the impact and compressive behavior of additively manufactured polyamide 6 (PA6) nanocomposite sandwich panels reinforced with amine‐functionalized graphene ...
Russo Swart   +3 more
wiley   +1 more source

Role of Fiber Sizing in Interfacial Relaxation, Water Uptake and Fatigue Properties of Acrylic‐Matrix Composites

open access: yesPolymer Composites, Volume 47, Issue 18, Page 16541-16555, 20 September 2026.
Characterisation of glass fibre reinforced acrylic with acrylic‐tailored or multi‐compatible sizing agents. ABSTRACT Fiber‐reinforced infusible acrylic monomer resins are of interest as recyclable alternatives to epoxy and other thermoset resin composites, but the novelty of these resins causes published studies on acrylic‐matrix composites to often ...
Machar Devine   +3 more
wiley   +1 more source

Microstructural and Fractographic Characterization of a Thermally Embrittled Nuclear Grade Steel: Part I - Annealing

open access: yesMaterials Research, 2002
A nuclear reactor pressure vessel steel was submitted to different annealing heat treatments aimed at simulating neutron irradiation damage. The obtained microstructures were mechanically tested with subsequent metallographic and fractographic ...
Tarpani José R.   +3 more
doaj  

Hydrogen‐Assisted Fracture of Iron‐Based Fe–Ni–Al Alloys

open access: yesAdvanced Engineering Materials, Volume 28, Issue 17, 9 September 2026.
Principal relations and fracture mechanisms of single‐phase and precipitate‐strengthened Fe–Ni–Al alloys subjected to prior electrochemical hydrogen charging are identified. The mechanisms of hydrogen effect on strength and microhardness are discussed, including hydrogen‐induced increase in microhardness and the role of hydrogen in fracture behavior ...
Nataliya Yadzhak   +3 more
wiley   +1 more source

AUTO-SHAPE ANALYSIS OF IMAGE TEXTURES IN FRACTOGRAPHY

open access: yesImage Analysis and Stereology, 2011
The aim of this study is to estimate the velocity of fatigue crack growth (crack growth rate - CGR) from the texture in SEM images of crack surfaces. A simple and quick method is based on fitting training images as a linear combination of several small ...
Hynek Lauschmann, Ivan Nedbal
doaj   +1 more source

Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales

open access: yesAdvanced Engineering Materials, Volume 28, Issue 17, 9 September 2026.
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik   +7 more
wiley   +1 more source