Results 211 to 220 of about 15,584 (255)
Some of the next articles are maybe not open access.

Fractography of Polymers

Abstract This article provides an overview of polymer fractography, with examples of various fracture surfaces created under diverse loading conditions. The focus is on the interpretation of polymer fracture-surface features in light of the unique viscoelastic nature of polymers.
Jericho Moll, Corissa Lee
openaire   +1 more source

Fractography of Fiberglass

1994
This paper discusses the applications and the limitations of the fractography technique as applied to the fiberglass industry. The main limitation of fractography originates from the fact that fibers of strength greater than about 2000 MPa shatter into multiple small fragments upon fracture rendering it impossible to capture the true fracture surfaces.
openaire   +1 more source

Fractography of Composites

2003
Abstract This article depicts typical fractographic features for a number of different composite materials, covering interlaminar and translaminar fracture characteristics in composite materials.
openaire   +1 more source

Mechanical behavior and fractography of graphite and boron carbide particulates reinforced A356 alloy hybrid metal matrix composites

Advanced Composites and Hybrid Materials, 2020
Pankaj R. Jadhav   +3 more
semanticscholar   +1 more source

Fractography of Concrete

Abstract This article presents a brief description of the fundamental characteristics of concrete and its constituents for understanding concrete fracture surfaces. It discusses the following two types of fractures: fractures induced in the laboratory and existing (service) fractures.
openaire   +1 more source

Influence of B4C Reinforcement Particles with Varying Sizes on the Tensile Failure and Fractography of LM29 Alloy Composites

Journal of Failure Analysis and Prevention, 2020
G. Prasad   +3 more
semanticscholar   +1 more source

Fractography of Nitinol

Abstract This article focuses on the fractography of Nitinol, a shape memory alloy of nickel and titanium, in superelastic biomedical applications, which primarily comprise drawn and/or laser-cut wire and tube components. Overload fracture, hydrogen embrittlement fracture, and fatigue fracture are discussed in detail.
Louis G. Malito   +4 more
openaire   +1 more source

Fractography basics

2015
Michael D. Hayes   +2 more
openaire   +1 more source

Deep learning-based semantic segmentation for morphological fractography

Engineering Fracture Mechanics
Keke Tang   +3 more
semanticscholar   +1 more source