Completion of evaluation of manufacturing processes for B/Al composites containing 0.2mm diameter boron fibers [PDF]
Four fabricators produced a total of 54 B/1100 Al, B/6061 Al, and B/2024 Al panels for evaluation. The 8 ply unidirectional, 45 to 50 volume percent, panels were made using 0.20 mm diameter boron fibers which were obtained from a single supplier.
Moore, T. J., Moorhead, P. E.
core +1 more source
X-ray Fractography and Its Application to Failure Analysis(
和幸 松井 +3 more
openalex
A preliminary characterization of the tensile and fatigue behavior of tungsten-fiber/Waspaloy-matrix composite [PDF]
A microstructural study and a preliminary characterization of the room temperature tensile and fatigue behavior of a continuous, tungsten fiber, Waspaloy-matrix composite was conducted.
Corner, Ralph E., Lerch, Brad A.
core +1 more source
Fractography and tensile strength of glass wool fibres
Majbritt Deichgræber Lund +1 more
openalex +2 more sources
Fractography Analysis of Monolithic Epoxy with Tailored Topography
Rasheed Atif, Fawad Inam
openalex +2 more sources
Characterization of failure processes in tungsten copper composites under fatigue loading conditions [PDF]
A fractographic and metallographic investigation was performed on specimens of a tungsten fiber reinforced copper matrix composite (9 vol percent), which had experienced fatigue failures at elevated temperatures.
Gabb, Timothy P. +2 more
core +1 more source
Impact of Silicon Carbide Particles Weight Percentage on the Microstructure, Mechanical Behaviour, and Fractography of Al2014 Alloy Composites [PDF]
Harikishor Kumar +6 more
openalex +1 more source
Mechanical Properties of Micro/Nanocellulose-Filled Epoxy Sheets at Subzero and Elevated Temperatures. [PDF]
Gulipalli P +3 more
europepmc +1 more source