Results 11 to 20 of about 7,770 (217)
The reconstitution of the history of a fatigue process is based on the knowledge of any correspondences between the morphology of the crack surface and the velocity of the crack growth (crack growth rate - CGR).
Hynek Lauschmann +3 more
doaj +4 more sources
Creep rupture properties of bare and coated polycrystalline nickel-based superalloy Rene®80 [PDF]
The mechanism governing de-oxidation of vanadium metal is regarded as fundamental knowledge; however, it has not been elucidated in existing literature.
Barjesteh M.M. +3 more
doaj +1 more source
Optimization of T-6 cycle and Characterization of Si3N4 Reinforced High Strength Aluminum Metal Matrix Composites [PDF]
In this research, AA7068/Si3N4 composites were fabricated through stir casting with the attachment of ultrasonic treatment. The quenching medium and aging duration significantly influenced the hardness of Al alloy samples.
Ashish Kumar +3 more
doaj +1 more source
The purpose of this study was to understand the behavior of martensitic H13 steel in accordance with the microstructural evolution, mechanical properties and wear in repeated tempering cycles.
Amitkumar Shelar, B. P. Ronge
doaj +1 more source
Forensic fractography of bone: fracture origins from impacts, and an improved understanding of the failure mechanism involved in beveling [PDF]
Fractography involves the study of fractures and cracks in a material in order to understand the cause of failure. Even as a complex, highly hierarchical composite, bone is a material that obeys physical laws, including cracking behavior.
Berryman, Hugh +8 more
core +1 more source
Today’s demand for environmentally friendly and energy-efficient solutions to the construction industry has driven researchers to match natural resources with traditional technics to develop new building technologies.
F. P. Teixeira +3 more
doaj +1 more source
Effect of Boride Layer on PM HSS AISI M2 on the Mechanisms Acting in the Transverse Rupture Strength Test [PDF]
Herein, it was conducted a study in order to examine the main fracture characteristics in the transverse rupture strength test (TRS) of a high speed steel (HSS) AISI M2 produced by powder metallurgy (PM) and with boriding treatment.
Mateus Leal Arcego +3 more
doaj +2 more sources
The paper presents results of the investigations on the effect of the low-temperature thermomechanical treatment on the microstructure of AlZn6Mg0.8Zr alloy (7003 alloy) and the relationships between microstructure and fatigue properties and fractography
Aleksander Kowalski +4 more
doaj +1 more source
Cauchy-based Modelling in Cementitious Materials Technology [PDF]
Cauchy paved the way for constructing models in concrete technology, and elsewhere. He determined the (nonflat) surface area in 3D by measuring random total projections. Analogously, he determined the length of a curved line in 2D by way of measuring the
P. Stroeven, M. Słowik
doaj +1 more source
Fractography and failure mechanisms of amorphous thermoplastics
S.387-436For glassy thermoplastics during the fracture process itself, craze material is differently formed and fractured depending on microscopic parameters such as molecular weight and on macroscopic prameters such as time, crack speed and stress ...
Döll, W.
core +1 more source