Fracture morphology of carbon fiber reinforced plastic composite laminates

open access: yesMaterials Research, 2010
Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications.
Vinod Srinivasa   +6 more
doaj   +1 more source

Experimental investigation of shape memory polymer hybrid nanocomposites modified by carbon fiber reinforced multi-walled carbon nanotube (MWCNT)

open access: yesMaterials Research Express, 2021
This paper presents the effect of the variations of multi-walled carbon nanotube (MWCNT) modification in shape memory polymer hybrid composites concerning their mechanical, thermomechanical, and shape memory characterizations.
Kanif Markad, Achchhe Lal
doaj   +1 more source

Coordinated Architectural and Chemical Reinforcement in the Crushing Mandible of a Soldier Termite

open access: yesAdvanced Functional Materials, EarlyView.
The crushing mandible of a soldier termite withstands substantial biting loads despite lacking mineral. Its cuticle is partitioned: convex teeth pair hardness and zinc enrichment with aligned chitin fibers for contact durability, while stiffer concave regions between teeth carry bending loads.
Andrew Tran Nguyen   +16 more
wiley   +1 more source

Wood Sawdust as a Low‐Cost Filler in Whole‐Tire Reclaimed Rubber: Mechanical Characterization and Factory‐Scale Cost Analysis

open access: yesJournal of Applied Polymer Science, EarlyView.
Whole‐tire reclaimed rubber is upgraded with wood sawdust, a carpentry by‐product available at no cost, across loadings from 0 to 20 wt%. At 5 wt%, tensile strength, elongation, hardness, viscosity, and water absorption all stay within commercial specification, and real factory data show an annual production saving near $62,000 with no capital ...
Mohammed S. Matar   +3 more
wiley   +1 more source

Study of the fractography and micromechanisms of near-threshold fatigue cracking and transgranular stress-corrosion cracking [PDF]

open access: yes, 1991
Micromechanisms and fractography of fatigue cracking -- Fractography and mechanisms of environment-assisted cracking -- Basic techniques for studying the fractography and crystallography of cracking -- The fractography of near-threshold fatigue cracking ...
Shiqiong, Li
core   +1 more source

Nonwoven rCF/PA6 Thermoplastic Composites: Hybrid Commingled Fibers vs. Powder Impregnation—Effects on Microstructure and Mechanical Properties

open access: yesPolymer Composites, EarlyView.
Comparison of powder impregnation and hybrid commingled non‐wovens for PA6/rCF nonwoven composites. The two‐step powder route gives lower voids and higher properties, while the single‐step hybrid route is limited by precursor inhomogeneity and high void content.
Gaia Francesca Lupia   +4 more
wiley   +1 more source

Study of fractography of ferritic ductile iron at different temperatures and loading conditions

open access: yesMaterials Research Express
This study characterizes the fractography of ferritic ductile iron under various loads, including tensile, fatigue and bending, and impact conditions. The results indicate that ductile fracture is the primary mechanism observed during tensile testing at ...
Wenjie Wang   +9 more
doaj   +1 more source

Impact of Fiber Treatments on the Properties and Aging Behavior of a Bio‐Composite Characterized From Nano‐ to Macro‐Scale

open access: yesPolymer Composites, EarlyView.
From Posidonia oceanica seagrass fibers to sustainable bio‐composites: the role of alkaline treatment in composite performance and durability. ABSTRACT The valorization of the abundant marine residue Posidonia oceanica (PO) fibers, as a filler in a bio‐based epoxy matrix was investigated.
Mahamat Saleh Elhadj Yacoub   +4 more
wiley   +1 more source

Tufting‐Based Manufacturing Method for High‐Performance 3D Composite Lap Joints

open access: yesPolymer Composites, EarlyView.
Graphical abstract illustrating the manufacturing process of a tufted non‐crimp preform lap joint, fractographic characterisation and comparative mechanical performance evaluation. ABSTRACT This study presents a tufting‐enabled through‐thickness reinforcement approach for enhancing the performance of 3D composite lap joints manufactured using resin ...
J. Ahmed   +3 more
wiley   +1 more source

Microscopic observation of creep-fatigue crack propagation in lead-free solder

open access: yesNihon Kikai Gakkai ronbunshu, 2015
Creep-fatigue crack propagation tests of lead-free solder were conducted under various loading waveforms. The waveforms adapted in displacement-controlled tests were four triangular waveforms: pp waveform having fast loading-unloading, cc waveform having
Keisuke TANAKA   +4 more
doaj   +1 more source