Results 101 to 110 of about 7,770 (217)
Correlative light-electron fractography of interlaminar fracture in a carbon-epoxy composite
This work evaluates the use of light microscopes (LMs) as a tool for interlaminar fracture of polymer composite investigation with the aid of correlative fractography.
Hein, Luis Rogerio de O. +3 more
core +1 more source
Applications of Fractography to Core and Outcrop Investigations
Purpose of this paper is to introduce geologists to the principles of fractography, especially those principles that govern the formation of fracture surface structures commonly observed in rocks.
Kulander, Byron R. +2 more
core +2 more sources
High-boron 9–10% chromium martensitic steels are an advanced material for manufacturing various com-ponents of thermal power units in coal-fired power plants operating under ultra-supercritical steam conditions (up to ...
Ivan S. Brazhnikov +1 more
doaj +1 more source
In present study, Metal Inert Gas (MIG) welding with ER309L austenitic filler wire was used to weld API X70 and SS 401 steel. This particular joint is mainly used in oil and gas plants where stainless steel need to be connected to the high strength low ...
Lochan Sharma +6 more
doaj +1 more source
This study investigates hydrogen-assisted fatigue crack growth (FCG) in vintage pipeline steels to quantify grade-dependent degradation under hydrogen–natural gas blending conditions.
Nayem Ahmed +3 more
doaj +1 more source
The investigation of structure and properties in the intermetallic compound Ni3Al, synthesized via self-propagating high-temperature synthesis (SHS-compaction) under quasi-volumetric thermal-explosion conditions, is presented in this study. The effect of
Kirill O. Akimov +2 more
doaj +1 more source
Fractography and Crack Initiation of Very-High-Cycle Fatigue for a High Carbon Low Alloy Steel
Very-High-Cycle Fatigue (VHCF) is the phenomenon of fatigue damage and failure of metallic materials or structures subjected to 108 cycles of fatigue loading and beyond.
钱桂安, 周承恩, 洪友士
core +2 more sources
In the failure analysis of metallic materials, the observation of fracture-surface morphology by scanning electron microscopy (SEM) is an important means of determining the fracture mechanisms.
Zhihui Li +5 more
doaj +1 more source
Microstructural changes and tensile fractography of Al-6061 after solutionizing and aging
This study investigates the effect of two-step heat treatment on the microstructure, mechanical properties, and fracture behavior of Al6061 alloy. Four conditions were examined: as-received and three heat-treated samples subjected to solution heat ...
Saurabh Dewangan +1 more
doaj +1 more source
Fractography, elastic modulus and oxidation resistance of novel metal-intermetallic Ni/Ni 3Al multilayer films [PDF]
Novel metal–intermetallic Ni/Ni3Al multilayer films are synthesized by a magnetron sputtering technique. The fractography, elastic modulus, and the oxidation resistance of the multilayer films are studied by a series of experimental tests.
Shen, H +4 more