Changes of Microstructures and Mechanical Properties in Commercially Pure Titanium after Different Cycles of Proposed Multi-Directional Forging

open access: yesMetals, 2019
A newly proposed multi-directional forging (MDF) was successfully applied to a commercially pure titanium (CP Ti). Severe plastic deformation would result in significant and complex changes of microstructure and mechanical properties, so microstructure ...
Zhanguang Zheng   +4 more
doaj   +1 more source

Effect of test temperature on low-cycle fatigue of high-chromium steel with high boron and low nitrogen content

open access: yesFrontier Materials & Technologies
High-boron 9–10% chromium martensitic steels are an advanced material for manufacturing various com-ponents of thermal power units in coal-fired power plants operating under ultra-supercritical steam conditions (up to ...
Ivan S. Brazhnikov   +1 more
doaj   +1 more source

Investigation of microstructure, corrosion, and mechanical properties of MIG welded API X70 and SS401 joints

open access: yesФізика і хімія твердого тіла
In present study, Metal Inert Gas (MIG) welding with ER309L austenitic filler wire was used to weld API X70 and SS 401 steel. This particular joint is mainly used in oil and gas plants where stainless steel need to be connected to the high strength low ...
Lochan Sharma   +6 more
doaj   +1 more source

Microstructural changes and tensile fractography of Al-6061 after solutionizing and aging

open access: yesMaterials Research Express
This study investigates the effect of two-step heat treatment on the microstructure, mechanical properties, and fracture behavior of Al6061 alloy. Four conditions were examined: as-received and three heat-treated samples subjected to solution heat ...
Saurabh Dewangan   +1 more
doaj   +1 more source

Investigation of the Static and Dynamic Mechanical Properties of the Base Metal and Weld Zone of Haynes 25 Alloy [PDF]

open access: yesIranian Journal of Materials Science and Engineering
This work presents a comprehensive investigation of the high cycle fatigue behavior of Haynes 25 cobalt-based superalloy and its welds produced by pulsed continuous-wave (CW) laser welding.
Mahdi Behjati   +2 more
doaj  

Mechanical characteristics and failure analysis of AA6082/TiC/graphene hybrid composites

open access: yesMaterials Research Express
The main aim of the present research is to improve the tensile strength of lightweight aluminium alloy 6082, which makes it fit for many advanced engineering applications.
Sohan Lal   +4 more
doaj   +1 more source