ABSTRACT In this study, the fracture response of polypropylene (PP) was assessed using J‐integral evaluation, J‐R curve construction, and fractography examination. J‐R and load–displacement curves were analyzed to determine critical loads and estimate J‐integral values based on standards established for polymer fracture testing, which led to the ...
N. Choupani +3 more
wiley +1 more source
Nondestructive Testing of Welded Composite Metal Foams
X‐ray computed tomography (CT) is used to evaluate welded steel–steel composite metal foam (CMF) joints of two density classes. It reports variation in postweld spatial void distribution and correlates it to weld‐induced changes, mechanical performance, and failure within welded CMF panels.
Chinmaya Prerana Inguva +2 more
wiley +1 more source
A nuclear reactor pressure vessel steel was submitted to different annealing heat treatments aimed at simulating neutron irradiation damage. The obtained microstructures were mechanically tested with subsequent metallographic and fractographic ...
Tarpani José R. +3 more
doaj
This study demonstrates how optimizing laser power, scanning speed, and hatching distance in laser powder bed fusion can boost the productivity of Inconel 718 manufacturing by up to 29% while maintaining mechanical integrity. The work delivers a validated process window and cost–time analysis, offering industry‐ready guidelines for efficient additive ...
Amir Behjat +7 more
wiley +1 more source
AUTO-SHAPE ANALYSIS OF IMAGE TEXTURES IN FRACTOGRAPHY
The aim of this study is to estimate the velocity of fatigue crack growth (crack growth rate - CGR) from the texture in SEM images of crack surfaces. A simple and quick method is based on fitting training images as a linear combination of several small ...
Hynek Lauschmann, Ivan Nedbal
doaj +1 more source
Additive manufacturing provides precise control over the placement of continuous fibres within polymer matrices, enabling customised mechanical performance in composite components. This article explores processing strategies, mechanical testing, and modelling approaches for additive manufactured continuous fibre‐reinforced composites.
Cherian Thomas, Amir Hosein Sakhaei
wiley +1 more source
Fatigue life of high strength steel for cold forming
The article presents the results of fatigue tests carried out on STRENX-type high-strength cold forming steel. For high-cycle fatigue tests carried out using low cycle loading frequencies of around 30 Hz, a ROTOFLEX machine was used. For ultra high-cycle
R. Ulewicz, F. Novy
doaj
A quasi‐periodic Dart‐Kite (QDK) metastructure with a golden‐ratio‐constrained strong–weak bond network simultaneously enhances strength, toughness, and damage tolerance. Its distributed topology enables predictable, tailorable crack paths for precise fracture control and stable mechanics, demonstrating a high‐performance, controllable architecture ...
Tianyu Gao +3 more
wiley +1 more source
Relationship between microstructure and fracture types in a UNS S32205 duplex stainless steel
Duplex stainless steels are susceptible to the formation of sigma phase at high temperature which could potentially be responsible for catastrophic service failure of components.
Maria Victoria Biezma +2 more
doaj
ABSTRACT Fe‐Cr‐Ni‐Cu alloy has been extensively utilized over the past few decades due to its low cost yet high strength. Nevertheless, the poor ductility of this alloy limits its real application in industrial fields. In this study, a soft Fe‐Cr‐Ni alloy was combined with a Fe‐Cr‐Ni‐Cu alloy by laser‐directed energy deposition (LDED) to fabricate the ...
Jiuxing Tang +9 more
wiley +1 more source