Results 71 to 80 of about 7,291 (217)

Fractography of Bone Using Reconstructed Computed Tomography (CT) Scans: A Case Report Series

open access: yes, 2022
Fractography has been shown to be applicable to forensic assessments of skeletal trauma by observing the presence and orientation of fracture surface features, which reveal information about the direction of crack propagation.
Decker, Summer, Christensen, Angi
core   +1 more source

Relationship between microstructure and fracture types in a UNS S32205 duplex stainless steel

open access: yesMaterials Research, 2013
Duplex stainless steels are susceptible to the formation of sigma phase at high temperature which could potentially be responsible for catastrophic service failure of components.
Maria Victoria Biezma   +2 more
doaj  

Role of Fiber Sizing in Interfacial Relaxation, Water Uptake and Fatigue Properties of Acrylic‐Matrix Composites

open access: yesPolymer Composites, Volume 47, Issue 18, Page 16541-16555, 20 September 2026.
Characterisation of glass fibre reinforced acrylic with acrylic‐tailored or multi‐compatible sizing agents. ABSTRACT Fiber‐reinforced infusible acrylic monomer resins are of interest as recyclable alternatives to epoxy and other thermoset resin composites, but the novelty of these resins causes published studies on acrylic‐matrix composites to often ...
Machar Devine   +3 more
wiley   +1 more source

Fractography of Long Bones with High-Velocity Projectile Trauma

open access: yes, 2020
Previous studies of bone fractography have examined only cases of blunt trauma. Here we assess whether fracture surface features are also found on bones subjected to high-velocity projectile trauma. Civil War–era long bones were assessed for the presence
Lillard, Kimberleigh, Christensen, Angi
core   +1 more source

Effects of Annealing Temperature on Microstructural Evolution and Mechanical Properties in Cold-Rolled High-Nitrogen Austenitic Steel

open access: yesMetals
High-nitrogen austenitic steel (HNS) cold-rolled with a reduction rate of 25% was subjected to an investigation of the effect of annealing temperature on microstructural evolution, tensile properties and the variation in fracture surface morphology.
Jong-Ho Shin   +2 more
doaj   +1 more source

Hydrogen‐Assisted Fracture of Iron‐Based Fe–Ni–Al Alloys

open access: yesAdvanced Engineering Materials, Volume 28, Issue 17, 9 September 2026.
Principal relations and fracture mechanisms of single‐phase and precipitate‐strengthened Fe–Ni–Al alloys subjected to prior electrochemical hydrogen charging are identified. The mechanisms of hydrogen effect on strength and microhardness are discussed, including hydrogen‐induced increase in microhardness and the role of hydrogen in fracture behavior ...
Nataliya Yadzhak   +3 more
wiley   +1 more source

Analisis Kegagalan Pada Bottle Gripper Dengan Mengunakan Metode Fractography (Studi Kasus Pt.Amarta Indah Otsuka) [PDF]

open access: yes, 2012
Terjadi kegagalan dari sebuah komponen dalam suatu mesin produksi minuman (PT. Amerta Indah Otsuka) bottle gripper yang merupakan komponen dari suatu mekanisme yang bertugas untuk mengangkat dan memindahkan bottle yang telah terisi.
Azarya,ArdyaJulio
core  

Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales

open access: yesAdvanced Engineering Materials, Volume 28, Issue 17, 9 September 2026.
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik   +7 more
wiley   +1 more source

Literature review on fractography of dental ceramics

open access: yes, 2022
치과용 세라믹의 파절실험 후 파절이 발생한 원인을 분석하면 세라믹의 임상적용 가능성을 높일 수 있다. 파절원인을 파악하기 위한 파단면분석은 주사전자현미경 등 영상기술의 발달로 점차 널리 적용되고 있는데 이를 정확히 해석하기 위해서는 실험조건 설정이 중요하다. 파절시편이 오염되지 않도록 보관하고 세척하며, 관찰을 위해 금속 전처리가 필요하다.
Chan-Jin Park   +5 more
core   +1 more source

Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A

open access: yesAdvanced Engineering Materials, Volume 28, Issue 17, 9 September 2026.
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han   +5 more
wiley   +1 more source