Hypochlorous acid as a potential cavity conditioner for caries-affected dentin. [PDF]
Sanon K +8 more
europepmc +1 more source
Polar Cryogenic Impact Behavior of Selective Laser Melted Ti-6Al-4V Alloy: Effects of Scanning Strategies and Notch Orientation. [PDF]
Chen H +6 more
europepmc +1 more source
GLARE teardowns from the MegaLiner Barrel (MLB) fatigue test [PDF]
, F.P., Grootema +14 more
core +1 more source
Pre-weld friction stir processing mitigates hot cracking and strengthens AA6061 fusion welds. [PDF]
Jalili A +4 more
europepmc +1 more source
A Comparison Between the Growth of Naturally Occurring Three-Dimensional Cracks in Scalmalloy<sup>®</sup> and Pre-Corroded 7085-T7452 and Its Implications for Additively Manufactured Limited-Life Replacement Parts. [PDF]
Peng D +6 more
europepmc +1 more source
Tailoring Microstructure and Performance of Cu/SiC Composites via Integrated Powder Metallurgy and Thermo-Compression Processing. [PDF]
Shan M +6 more
europepmc +1 more source
Study on the Transverse Properties of T800-Grade Unidirectional Carbon Fiber-Reinforced Polymers. [PDF]
Wang H +9 more
europepmc +1 more source
Indentation Fractography: A Measure of Brittleness
Brian R. Lawn, David B. Marshall
openalex +1 more source
Tensile deformation and fracture properties of a 14YWT nanostructured ferritic alloy [PDF]
Alam +33 more
core +1 more source