Results 51 to 60 of about 2,320 (181)

In Vitro Mechanical Tests for Modern Dental Ceramics

open access: yesFrontiers in Dentistry, 2006
The fracture resistance of all-ceramic restorations is one of the major concerns in clinical applications of these materials. Before initiating a time-consuming and costly clinical investigation, an in vitro study can help to estimate the in vivo ...
L. Sadighpour   +2 more
doaj  

Improvement of experimental device for high cycle fatigue tests of copper alloy strips and characterizing fatigue properties

open access: yesNihon Kikai Gakkai ronbunshu, 2021
In this research, we improved the fatigue test method for copper alloy strips which was standardized by Japan Copper and Brass Association. In order to increase test frequency and obtain repeatable test results for 108 cycles, the design of fixed block ...
Natsuhiro MITA   +2 more
doaj   +1 more source

Fracture load and three‐dimensional internal void analysis of direct composites used to restore worn molars

open access: yesEuropean Journal of Oral Sciences, EarlyView.
Abstract This study evaluated (1) the load‐bearing capacity of molars restored with direct occlusal veneers fabricated either from short‐fiber‐reinforced composite (SFRC) or particulate‐filled composite (PFC) and the presence of internal voids within the materials, and (2) effect of water storage on the fracture load and correlation between internal ...
Topias Yli‐Urpo   +6 more
wiley   +1 more source

Indirect Tensile Test of Layered Marble and Analysis of Fracture Morphology and Mechanism

open access: yes工程科学与技术, 2014
:With the aid of MTS815,large scale laser profilometer and SEM testing system,indirect tensile tests,fractography and meso fracture mechanism analysis were carried out on layered marbles taken from transportation tunnel of JinpinⅡ hydropower station ...
裴建良, 苏立, 刘建锋, 左建平
doaj  

Biography of Are Tsirk (1937-2015): Flintknapper and scholar

open access: yesJournal of Lithic Studies, 2015
Are Tsirk was as much a scholar as he was a flintknapper. These disciplines were intertwined and expressed in his experimental research, by way of his exploration of fractography, and his replication of stone tools which spanned the archaeological record
Steve Adams
doaj   +1 more source

Breakage Characterization of Magnetite under Impact Loads and Cyclic Impact Loading

open access: yesEnergies, 2020
A series of impact compression tests were conducted to study the breakage characteristics of magnetite, as well as the impact pressure on its strain rate and dynamic compressive strength.
Liang Si, Yijun Cao, Guixia Fan
doaj   +1 more source

Effect of substructure fabrication method and design on the fracture resistance properties of metal–ceramic restorations

open access: yesJournal of Prosthodontics, EarlyView.
Abstract Purpose In metal–ceramic restorations, the substructure fabrication method and design may affect the prognosis of the prosthesis. This study evaluated and compared the fracture resistance of metal–ceramic restorations fabricated with different substructure fabrication methods using two different alloy powders and designs.
Young‐Hoon Lee   +4 more
wiley   +1 more source

Fractographic Analysis Of Selected Boron Steels Subjected To Impact Testing

open access: yesArchives of Metallurgy and Materials, 2015
In this paper dynamic properties of low-alloy boron steels – Hardox 500, B27 and HTK 900H in delivered state (after hardening and tempering) are considered.
Dudziński W.   +2 more
doaj   +1 more source

Structural characterization and optimum machining parameters of jute/carbon fibre hybrid reinforced epoxy composite laminates

open access: yesPolymer International, Volume 75, Issue 9, Page 804-817, September 2026.
Hybrid jute/carbon epoxy laminates have better mechanical performance and less drilling damage by the use of optimized stacking sequence and machining parameters. Abstract Three composite laminate systems were produced using the standard hand lay‐up method: jute‐fibre‐reinforced polymer (JFRP), carbon‐fibre‐reinforced polymer (CFRP) and a hybrid of the
Paulraj Prabhu   +5 more
wiley   +1 more source

Failure Investigation of Alloy 625 Sockolets After Prolonged Service in an Ammonia Cracker Unit

open access: yesMaterials and Corrosion, Volume 77, Issue 8, Page 1375-1384, August 2026.
The failure of the sockolets was caused by intergranular cracking and fracture. The thick and highly brittle nitrided layer formed intergranular surface cracks, which propagated along grain boundaries into the base alloy substrate due to the presence of brittle Cr‐rich carbides. ABSTRACT Several sockolets of Alloy 625 operating at 540°C in contact with
Kamlesh Chandra   +2 more
wiley   +1 more source