Results 91 to 100 of about 8,376 (173)

Fractography and Crack Initiation of Very-High-Cycle Fatigue for a High Carbon Low Alloy Steel

open access: yes, 2006
Very-High-Cycle Fatigue (VHCF) is the phenomenon of fatigue damage and failure of metallic materials or structures subjected to 108 cycles of fatigue loading and beyond.
钱桂安, 周承恩, 洪友士
core   +2 more sources

Investigation of microstructure, corrosion, and mechanical properties of MIG welded API X70 and SS401 joints

open access: yesФізика і хімія твердого тіла
In present study, Metal Inert Gas (MIG) welding with ER309L austenitic filler wire was used to weld API X70 and SS 401 steel. This particular joint is mainly used in oil and gas plants where stainless steel need to be connected to the high strength low ...
Lochan Sharma   +6 more
doaj   +1 more source

Applications of Fractography to Core and Outcrop Investigations

open access: yes, 1979
Purpose of this paper is to introduce geologists to the principles of fractography, especially those principles that govern the formation of fracture surface structures commonly observed in rocks.
Kulander, Byron R.   +2 more
core   +2 more sources

Relationship between microstructure and fracture types in a UNS S32205 duplex stainless steel

open access: yesMaterials Research, 2013
Duplex stainless steels are susceptible to the formation of sigma phase at high temperature which could potentially be responsible for catastrophic service failure of components.
Maria Victoria Biezma   +2 more
doaj  

Effect of test temperature on low-cycle fatigue of high-chromium steel with high boron and low nitrogen content

open access: yesFrontier Materials & Technologies
High-boron 9–10% chromium martensitic steels are an advanced material for manufacturing various com-ponents of thermal power units in coal-fired power plants operating under ultra-supercritical steam conditions (up to ...
Ivan S. Brazhnikov   +1 more
doaj   +1 more source

Microstructural changes and tensile fractography of Al-6061 after solutionizing and aging

open access: yesMaterials Research Express
This study investigates the effect of two-step heat treatment on the microstructure, mechanical properties, and fracture behavior of Al6061 alloy. Four conditions were examined: as-received and three heat-treated samples subjected to solution heat ...
Saurabh Dewangan   +1 more
doaj   +1 more source

A Lightweight Classification Method Based on You Only Look Once Version 8 and Convolutional Block Attention for Scanning Electron Microscopy Images of Metal Fracture Surfaces

open access: yesCrystals
In the failure analysis of metallic materials, the observation of fracture-surface morphology by scanning electron microscopy (SEM) is an important means of determining the fracture mechanisms.
Zhihui Li   +5 more
doaj   +1 more source

Fractography, elastic modulus and oxidation resistance of novel metal-intermetallic Ni/Ni 3Al multilayer films [PDF]

open access: yes, 2002
Novel metal–intermetallic Ni/Ni3Al multilayer films are synthesized by a magnetron sputtering technique. The fractography, elastic modulus, and the oxidation resistance of the multilayer films are studied by a series of experimental tests.
Shen, H   +4 more
core  

Textural fractography of fatigue failures under variable cycle loading

open access: yes, 2005
A new concept of counting time at fatigue processes is proposed, aimed to reach fractographic compatibility in cases of different loading sequences. Values of cycle effectivity are summarized to give the new reference time.
H Lauschmann (13713577)   +2 more
core  

The Fractography of Bone: Impact of Flat Bone and the Story It Tells [PDF]

open access: yes
Fractography as a method for fracture analysis has been applied widely to materials that range from glass to ceramics and polymers of varying compositions. Very limited research has been done, however, to apply this knowledge of fractography and fracture
Mendoza, Brandon   +7 more