Fractography of Nitinol

Abstract This article focuses on the fractography of Nitinol, a shape memory alloy of nickel and titanium, in superelastic biomedical applications, which primarily comprise drawn and/or laser-cut wire and tube components. Overload fracture, hydrogen embrittlement fracture, and fatigue fracture are discussed in detail.
Louis G. Malito   +4 more
openaire   +1 more source

Fractography basics

2015
Michael D. Hayes   +2 more
openaire   +1 more source

Fractography of clinical failures of indirect resin composite endocrown and overlay restorations

Dental Materials, 2021
Susanne Scherrer   +2 more
exaly  

Quantitative fractography for brittle fracture via multilayer perceptron neural network

Engineering Fracture Mechanics, 2023
Lingyue Ma   +2 more
exaly  

History of Fractography

Abstract This article reviews the historical development of fractography, from the early studies of fracture appearance dating back to the sixteenth century, and including the development of microfractography in the middle of the 20th century, to the current state-of-the-art work in electron fractography and quantitative fractography.
openaire   +1 more source

Fracture and Fractography

2003
Abstract This article introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination and ...
openaire   +1 more source

Elements of Fractography

2018
This chapter begins with a description of the different classifications of fracture, according to mechanism and extent of plastic deformation. The mechanical aspects of fracture, from the continuum mechanics and fracture mechanics points of view, are briefly described.
openaire   +1 more source

Formability and fractography of AA5754/polyethylene/AA5754 sandwich composites

Mechanics Based Design of Structures and Machines, 2022
Ramin Hashemi, Seyed Ali Niknam
exaly  

ADM guidance—Ceramics: guidance to the use of fractography in failure analysis of brittle materials

Dental Materials, 2017
Paulo Francisco Cesar   +2 more