Possibilities of Fractography

Metal Science and Heat Treatment, 2005
A brief characteristic of methods of observation, measurement, identification, and analysis of fractures is presented. Prospects of the use of the methods of fractography for solving problems of certification of materials, determining the structural mechanisms of fracture, and controlling the quality of metals are discussed.
openaire   +1 more source

Fractography of Concrete

Abstract This article presents a brief description of the fundamental characteristics of concrete and its constituents for understanding concrete fracture surfaces. It discusses the following two types of fractures: fractures induced in the laboratory and existing (service) fractures.
openaire   +1 more source

Fractography basics

2015
Michael D. Hayes   +2 more
openaire   +1 more source

Elements of Fractography

2018
This chapter begins with a description of the different classifications of fracture, according to mechanism and extent of plastic deformation. The mechanical aspects of fracture, from the continuum mechanics and fracture mechanics points of view, are briefly described.
openaire   +1 more source

Quantitative Fractography for Brittle Fracture via Multilayer Perceptron Neural Network

Engineering Fracture Mechanics, 2023
Lingyue Ma   +2 more
exaly  

Fracture and Fractography

2003
Abstract This article introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination and ...
openaire   +1 more source

History of Fractography

Abstract This article reviews the historical development of fractography, from the early studies of fracture appearance dating back to the sixteenth century, and including the development of microfractography in the middle of the 20th century, to the current state-of-the-art work in electron fractography and quantitative fractography.
openaire   +1 more source

Forensic Fractography of Bone Using Computed Tomography (CT) Scans

Journal of Forensic Radiology and Imaging, 2019
Angi M Christensen, Gary M Hatch
exaly  

Fractography and Failure Analysis

Structural Integrity, 2018
Jorge L Gonzalez-Velazquez