Results 221 to 230 of about 15,584 (255)
Some of the next articles are maybe not open access.
Formability and fractography of AA5754/polyethylene/AA5754 sandwich composites
Mechanics Based Design of Structures and Machines, 2022Ramin Hashemi, Seyed Ali Niknam
exaly
Abstract This article reviews the historical development of fractography, from the early studies of fracture appearance dating back to the sixteenth century, and including the development of microfractography in the middle of the 20th century, to the current state-of-the-art work in electron fractography and quantitative fractography.
openaire +1 more source
openaire +1 more source
2003
Abstract This article introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination and ...
openaire +1 more source
Abstract This article introduces the subject of fractography and how it is used in failure analysis. The discussion covers the structure of and fracture and crack-propagation behavior of polymeric materials, the distinction between the ductile and brittle fracture modes on the basis of macroscopic appearance, and the examination and ...
openaire +1 more source
2018
This chapter begins with a description of the different classifications of fracture, according to mechanism and extent of plastic deformation. The mechanical aspects of fracture, from the continuum mechanics and fracture mechanics points of view, are briefly described.
openaire +1 more source
This chapter begins with a description of the different classifications of fracture, according to mechanism and extent of plastic deformation. The mechanical aspects of fracture, from the continuum mechanics and fracture mechanics points of view, are briefly described.
openaire +1 more source
Deep Learning Based Dimple Segmentation for Quantitative Fractography
ICPR Workshops, 2020Ashish Sinha, K. Suresh
semanticscholar +1 more source
Fractography of zirconia-specimens made using additive manufacturing (LCM) technology
, 2017W. Harrer +3 more
semanticscholar +1 more source