Results 31 to 40 of about 7,291 (217)
Fracture morphology of carbon fiber reinforced plastic composite laminates
Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications.
Vinod Srinivasa +6 more
doaj +1 more source
This paper presents the effect of the variations of multi-walled carbon nanotube (MWCNT) modification in shape memory polymer hybrid composites concerning their mechanical, thermomechanical, and shape memory characterizations.
Kanif Markad, Achchhe Lal
doaj +1 more source
Coordinated Architectural and Chemical Reinforcement in the Crushing Mandible of a Soldier Termite
The crushing mandible of a soldier termite withstands substantial biting loads despite lacking mineral. Its cuticle is partitioned: convex teeth pair hardness and zinc enrichment with aligned chitin fibers for contact durability, while stiffer concave regions between teeth carry bending loads.
Andrew Tran Nguyen +16 more
wiley +1 more source
BSA addition to physiological solutions enhances resistance of a Zn alloy to stress corrosion cracking (SCC) but reduces its corrosion resistance. Extended surface characterization explains the contrasting influences on corrosion and SCC. Unexpectedly, the alloy suffers transgranular SCC (TGSCC), despite extensive grain boundary precipitation. Thorough
RK Singh Raman +9 more
wiley +1 more source
Fractography is the study of fracture surface morphology, and it can be used to assess a material’s mechanical properties as well as to determine the underlying mechanisms leading to material failure.
Maureen Bottrell +11 more
core +1 more source
Study of the fractography and micromechanisms of near-threshold fatigue cracking and transgranular stress-corrosion cracking [PDF]
Micromechanisms and fractography of fatigue cracking -- Fractography and mechanisms of environment-assisted cracking -- Basic techniques for studying the fractography and crystallography of cracking -- The fractography of near-threshold fatigue cracking ...
Shiqiong, Li
core +1 more source
To address functionality limitations in plant‐based and industrially compostable polymer aerogels, this work introduces bio‐inspired aerogels with broadened functionality. Inspired by functional plant tissues, lightweight biopolymer aerogels based on exclusively stereocomplex crystals are fabricated, featuring hierarchically macro‐/meso‐porous ...
Anthony V. Tuccitto +10 more
wiley +1 more source
Study of fractography of ferritic ductile iron at different temperatures and loading conditions
This study characterizes the fractography of ferritic ductile iron under various loads, including tensile, fatigue and bending, and impact conditions. The results indicate that ductile fracture is the primary mechanism observed during tensile testing at ...
Wenjie Wang +9 more
doaj +1 more source
Comparison of powder impregnation and hybrid commingled non‐wovens for PA6/rCF nonwoven composites. The two‐step powder route gives lower voids and higher properties, while the single‐step hybrid route is limited by precursor inhomogeneity and high void content.
Gaia Francesca Lupia +4 more
wiley +1 more source
From Posidonia oceanica seagrass fibers to sustainable bio‐composites: the role of alkaline treatment in composite performance and durability. ABSTRACT The valorization of the abundant marine residue Posidonia oceanica (PO) fibers, as a filler in a bio‐based epoxy matrix was investigated.
Mahamat Saleh Elhadj Yacoub +4 more
wiley +1 more source