Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A

open access: yesAdvanced Engineering Materials, EarlyView.
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han   +5 more
wiley   +1 more source

Coordinated Architectural and Chemical Reinforcement in the Crushing Mandible of a Soldier Termite

open access: yesAdvanced Functional Materials, EarlyView.
The crushing mandible of a soldier termite withstands substantial biting loads despite lacking mineral. Its cuticle is partitioned: convex teeth pair hardness and zinc enrichment with aligned chitin fibers for contact durability, while stiffer concave regions between teeth carry bending loads.
Andrew Tran Nguyen   +16 more
wiley   +1 more source

Study of fractography of ferritic ductile iron at different temperatures and loading conditions

open access: yesMaterials Research Express
This study characterizes the fractography of ferritic ductile iron under various loads, including tensile, fatigue and bending, and impact conditions. The results indicate that ductile fracture is the primary mechanism observed during tensile testing at ...
Wenjie Wang   +9 more
doaj   +1 more source

Wood Sawdust as a Low‐Cost Filler in Whole‐Tire Reclaimed Rubber: Mechanical Characterization and Factory‐Scale Cost Analysis

open access: yesJournal of Applied Polymer Science, EarlyView.
Whole‐tire reclaimed rubber is upgraded with wood sawdust, a carpentry by‐product available at no cost, across loadings from 0 to 20 wt%. At 5 wt%, tensile strength, elongation, hardness, viscosity, and water absorption all stay within commercial specification, and real factory data show an annual production saving near $62,000 with no capital ...
Mohammed S. Matar   +3 more
wiley   +1 more source

Nonwoven rCF/PA6 Thermoplastic Composites: Hybrid Commingled Fibers vs. Powder Impregnation—Effects on Microstructure and Mechanical Properties

open access: yesPolymer Composites, EarlyView.
Comparison of powder impregnation and hybrid commingled non‐wovens for PA6/rCF nonwoven composites. The two‐step powder route gives lower voids and higher properties, while the single‐step hybrid route is limited by precursor inhomogeneity and high void content.
Gaia Francesca Lupia   +4 more
wiley   +1 more source

Microscopic observation of creep-fatigue crack propagation in lead-free solder

open access: yesNihon Kikai Gakkai ronbunshu, 2015
Creep-fatigue crack propagation tests of lead-free solder were conducted under various loading waveforms. The waveforms adapted in displacement-controlled tests were four triangular waveforms: pp waveform having fast loading-unloading, cc waveform having
Keisuke TANAKA   +4 more
doaj   +1 more source

Microstructure, mechanical response and fractography of AZ91E/Al2O3 (p) nano composite fabricated by semi solid stir casting method

open access: yes, 2017
The present study confers to the fabrication and its characterization of magnesium alloy (AZ91E) based nano composites with nano Al 2 O 3 particulate reinforcements.
D. S. Kumar   +5 more
semanticscholar   +1 more source

Impact and Compressive Performance of 3D‐Printed PA6/Functionalized Graphene Nanoplatelet Sandwich Structures With Auxetic Cores

open access: yesPolymer Composites, EarlyView.
Schematic of PA6/functionalized graphene nanoplatelet compounding and filament extrusion to 3D printing, sandwich panel fabrication, and mechanical characterization. ABSTRACT This study examines the impact and compressive behavior of additively manufactured polyamide 6 (PA6) nanocomposite sandwich panels reinforced with amine‐functionalized graphene ...
Russo Swart   +3 more
wiley   +1 more source

Fracturing behavior of brittle solids containing 3D internal crack of different depths under ultrasonic fracturing

open access: yesInternational Journal of Mining Science and Technology, 2022
Ultrasonic fracturing (UF) can be used to form crack networks for oil or gas in the mining industry and hard rock excavation. In this paper, the three-dimensional internal laser-engraved crack method (3D-ILC) is introduced to make penny-shaped internal ...
Haijun Wang   +4 more
doaj   +1 more source

Role of Fiber Sizing in Interfacial Relaxation, Water Uptake and Fatigue Properties of Acrylic‐Matrix Composites

open access: yesPolymer Composites, EarlyView.
Characterisation of glass fibre reinforced acrylic with acrylic‐tailored or multi‐compatible sizing agents. ABSTRACT Fiber‐reinforced infusible acrylic monomer resins are of interest as recyclable alternatives to epoxy and other thermoset resin composites, but the novelty of these resins causes published studies on acrylic‐matrix composites to often ...
Machar Devine   +3 more
wiley   +1 more source