Temperature and load-ratio dependent fatigue-crack growth in the CrMnFeCoNi high-entropy alloy [PDF]
Multiple-principal element alloys known as high-entropy alloys have rapidly been gaining attention for the vast variety of compositions and potential combinations of properties that remain to be explored. Of these alloys, one of the earliest, the ‘Cantor
George, EP +5 more
core
Abstract This study evaluated (1) the load‐bearing capacity of molars restored with direct occlusal veneers fabricated either from short‐fiber‐reinforced composite (SFRC) or particulate‐filled composite (PFC) and the presence of internal voids within the materials, and (2) effect of water storage on the fracture load and correlation between internal ...
Topias Yli‐Urpo +6 more
wiley +1 more source
Relationship between microstructure and fracture types in a UNS S32205 duplex stainless steel
Duplex stainless steels are susceptible to the formation of sigma phase at high temperature which could potentially be responsible for catastrophic service failure of components.
Maria Victoria Biezma +2 more
doaj
This work presents, for the first time, an in-depth investigation of the structure–property–fatigue relationships of an Al-Mg-Si alloy (AA6061) processed via additive friction stir-deposition (AFS-D).
Ben A. Rutherford +7 more
doaj +1 more source
Improved silicon nitride for advanced heat engines [PDF]
The results of a four year program to improve the strength and reliability of injection-molded silicon nitride are summarized. Statistically designed processing experiments were performed to identify and optimize critical processing parameters and ...
Fang, Ho T., Yeh, Harry C.
core +1 more source
ABSTRACT In this study, the fracture response of polypropylene (PP) was assessed using J‐integral evaluation, J‐R curve construction, and fractography examination. J‐R and load–displacement curves were analyzed to determine critical loads and estimate J‐integral values based on standards established for polymer fracture testing, which led to the ...
N. Choupani +3 more
wiley +1 more source
High-nitrogen austenitic steel (HNS) cold-rolled with a reduction rate of 25% was subjected to an investigation of the effect of annealing temperature on microstructural evolution, tensile properties and the variation in fracture surface morphology.
Jong-Ho Shin +2 more
doaj +1 more source
The α and prior β textures and microtextures of a lamellar Ti6242 forged disk were characterized by advanced electron back scattered diffraction (EBSD) and related to crystallographic features of faceted crack initiation sites of dwell fatigue specimens ...
Lionel Germain +4 more
doaj +1 more source
Correlation of processing and sintering variables with the strength and radiography of silicon nitride [PDF]
A sintered Si3N4-SiO2-Y2O3 composition, NASA 6Y, was developed that reached four-point flexural average strength/standard deviation values of 857/36, 544/33, and 462/59 MPa at room temperature, 1200 and 1370 C respectively.
Baaklini, G. Y., Sanders, W. A.
core +1 more source
Abstract Purpose In metal–ceramic restorations, the substructure fabrication method and design may affect the prognosis of the prosthesis. This study evaluated and compared the fracture resistance of metal–ceramic restorations fabricated with different substructure fabrication methods using two different alloy powders and designs.
Young‐Hoon Lee +4 more
wiley +1 more source