Effects of Annealing on the Thermomechanical Properties and Crystallization Behavior of FDM‐Printed High‐Temperature PLA and Glass Fiber PLA Composites

open access: yesPolymer Engineering &Science, EarlyView.
Overview of the study evaluating the impact of post‐print annealing on the microstructural crystallization and thermomechanical properties of FDM‐printed high‐temperature PLA and glass fiber‐reinforced PLA composites. ABSTRACT Polylactic acid (PLA) combines renewable sourcing and reliable printability with limited stiffness retention near its glass ...
Huseyin Erdem Yalkin, Ayse Nur Ozkan
wiley   +1 more source

Microstructure, Defects, and Fatigue Response of High‐Strength Tool Steels

open access: yessteel research international, EarlyView.
The martensitic tool steel family is designed for use in various working environments where they are subjected to repeatedly high mechanical loads. Despite the continuous upgrade of material´s microstructures through compositional development or processing techniques, defects remain a critical factor for the tool performance by leading to fatigue ...
Katerina Chantziara   +3 more
wiley   +1 more source

Fractography used with lifetime prediction tests on commercial grades of alumina and silicon carbide

open access: yes, 1996
Fractographic investigations were conducted on alumina and α-SSiC bend bars from a round robin test comparing a static and a dynamic lifetime test method.
Woodtli, Jarmila (author)   +2 more
core   +1 more source

Fracturing behavior of brittle solids containing 3D internal crack of different depths under ultrasonic fracturing

open access: yesInternational Journal of Mining Science and Technology, 2022
Ultrasonic fracturing (UF) can be used to form crack networks for oil or gas in the mining industry and hard rock excavation. In this paper, the three-dimensional internal laser-engraved crack method (3D-ILC) is introduced to make penny-shaped internal ...
Haijun Wang   +4 more
doaj   +1 more source

Microstructure, mechanical response and fractography of AZ91E/Al2O3 (p) nano composite fabricated by semi solid stir casting method

open access: yes, 2017
The present study confers to the fabrication and its characterization of magnesium alloy (AZ91E) based nano composites with nano Al 2 O 3 particulate reinforcements.
D. S. Kumar   +5 more
semanticscholar   +1 more source

Multi‐Scale Mechanical Behavior of Additive‐Manufactured 316L Stainless Steel Processed by Severe Plastic Deformation

open access: yessteel research international, EarlyView.
The multi‐scale mechanical behavior of additive‐manufactured 316L stainless steel processed by directed energy deposition and high‐pressure torsion is explored. The influence of torsional strain on strength and microstructural evolution is revealed, indicating progressive grain refinement in the ultrafine regime, reaching strength levels nearing 1800 ...
M. Farhan Raza, Guney Guven Yapici
wiley   +1 more source

Fractography of polytetrafluoroethylene /PTFE/ [PDF]

open access: yes, 1968
Application of fractography to polymeric material using ...
Nerren, B. H.
core  

Multiscale fatigue damage characterization in short glass fiber reinforced polyamide-66 [PDF]

open access: yes, 2014
This paper aims at studying fatigue damage behavior of injection molded 30 wt% short glass fiber reinforced polyamide-66 composite (PA66/GF30). The evolution of dynamic modulus, hysteresis area, cyclic creep and temperature during fatigue tests were ...
ARIF, Muhamad Fatikul   +5 more
core   +1 more source

Characterization and Tensile Fractography of Nano ZrO2 Reinforced Copper-Zinc Alloy Composites

open access: yesFrattura ed Integrità Strutturale, 2019
Nano particulates fortified metal lattice composites are finding extensive variety of utilizations in car and sports hardware fabricating businesses. In the present investigation, an endeavor has been made to create copper-zinc-nano ZrO2 particulates ...
Madeva Nagaral   +3 more
semanticscholar   +1 more source

Improving fatigue resistance of translucent 4Y‐PSZ zirconia through glass gradation

open access: yesEuropean Journal of Oral Sciences, EarlyView.
Abstract To evaluate the effect of graded glass infiltration on the fatigue behavior and mechanical reliability of translucent 4Y‐PSZ zirconia before and after hydrothermal aging, disc‐shaped specimens were fabricated by uniaxial pressing and divided into control and glass‐graded groups (n = 36/group).
Felipe Machado Souza   +12 more
wiley   +1 more source