Results 41 to 50 of about 6,333 (218)
Herein, the stress corrosion cracking (SCC) susceptibility of duplex (UNS S32205) and austenitic (UNS S31653) stainless steel (SS) reinforcements was evaluated using integrity assessment criteria.
Ulises Martin, David M. Bastidas
doaj +1 more source
Fracture morphology of carbon fiber reinforced plastic composite laminates
Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications.
Vinod Srinivasa +6 more
doaj +1 more source
This paper presents the effect of the variations of multi-walled carbon nanotube (MWCNT) modification in shape memory polymer hybrid composites concerning their mechanical, thermomechanical, and shape memory characterizations.
Kanif Markad, Achchhe Lal
doaj +1 more source
Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik +7 more
wiley +1 more source
Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han +5 more
wiley +1 more source
Fractography of self-glazed zirconia with improved reliability
The fractography of a new grade of zirconia ceramics, known as self-glazed zirconia, was investigated. The as-sintered intact top surface was made with superior smoothness that mimicked the optical appearances of the natural teeth enamel.
Andraž Kocjan +26 more
core +1 more source
Investigating accidents involving aircraft manufactured from polymer composite materials [PDF]
This thesis looks into the examination of polymer composite wreckage from the perspective of the aircraft accident investigator. It develops an understanding of the process of wreckage examination as well as identifying the potential for visual and ...
Dunn, Leigh
core +2 more sources
This article investigates the dependence of the properties on the manufacturing orientation in the form of the inclination angle to the build plate of LPBF‐fabricated NiTi rods with a diameter of 150–220 µm. Metallographic, chemical, thermal, and mechanical characterization show behavior under identical manufacturing conditions that ranges from ...
Sandra Herzig +2 more
wiley +1 more source
Study of fractography of ferritic ductile iron at different temperatures and loading conditions
This study characterizes the fractography of ferritic ductile iron under various loads, including tensile, fatigue and bending, and impact conditions. The results indicate that ductile fracture is the primary mechanism observed during tensile testing at ...
Wenjie Wang +9 more
doaj +1 more source
Coordinated Architectural and Chemical Reinforcement in the Crushing Mandible of a Soldier Termite
The crushing mandible of a soldier termite withstands substantial biting loads despite lacking mineral. Its cuticle is partitioned: convex teeth pair hardness and zinc enrichment with aligned chitin fibers for contact durability, while stiffer concave regions between teeth carry bending loads.
Andrew Tran Nguyen +16 more
wiley +1 more source