Results 81 to 90 of about 5,804 (225)

Fractography analysis of Inconel 718 fatigued at 700°C

open access: yes, 2016
This work deals with the fractography analysis of nickel-base superalloy Inconel 718 fatigued at 700°C in air atmosphere in the high cycle region. During cyclic loading of this alloy at high temperatures some different mechanisms compared to cyclic ...
Otakar Bokůvka   +7 more
core   +1 more source

Quantitative prediction of fracture toughness (KIc) of polymer by fractography using deep neural networks

open access: yes, 2022
Fracture surfaces provide various types of information about fracture. The fracture toughness $${K_{{\rm{I}}c}}$$, which represents the resistance to fracture, can be estimated using the three-dimensional (3D) information of a fracture surface, i.e.
K. Ito, M. Demura, Y. Mototake
core   +1 more source

Failure Analysis of 316L Air Cooler Stainless Steel Tube in a Natural Gas Production Field

open access: yesInternational Journal of Electrochemical Science, 2015
In spite of the excellent resistance of stainless steel (SS) towards uniform corrosion, overcoming various localized corrosion could be a real challenge. This work presents an analysis of the failure behavior of 316L SS air chiller tube with a peripheral
A. Bahgat Radwan   +4 more
doaj   +1 more source

Use of the helium ion microscope in small crack fractography

open access: yes, 2022
Highly stressed aerospace structures, such as the wing attachment points and load carry-through bulkheads of fighter aircraft, often grow fatigue cracks from micro-scale discontinuities.
Jie Tian (20496)   +3 more
core  

Fractography of fatigue fractures : common features in different image textures

open access: yes, 2005
Fractography of fatigue fractures : common features in different image ...
J Sumbera (13734631)   +3 more
core  

Fractography and Crack Initiation of Very-High-Cycle Fatigue for a High Carbon Low Alloy Steel

open access: yes, 2006
Very-High-Cycle Fatigue (VHCF) is the phenomenon of fatigue damage and failure of metallic materials or structures subjected to 108 cycles of fatigue loading and beyond.
钱桂安, 周承恩, 洪友士
core  

Synergistic effects of cold rolling and age hardening on the hardness and tensile characteristics of AA6061 hybrid composites

open access: yesMaterials Research Express
The present study involves the fabrication of aluminium alloy 6061 matrix hybrid composites with varying weight fractions of silica sand and copper particles by employing the conventional stir casting method.
Ramakrishna Vikas Sadanand   +2 more
doaj   +1 more source

Changes of Microstructures and Mechanical Properties in Commercially Pure Titanium after Different Cycles of Proposed Multi-Directional Forging

open access: yesMetals, 2019
A newly proposed multi-directional forging (MDF) was successfully applied to a commercially pure titanium (CP Ti). Severe plastic deformation would result in significant and complex changes of microstructure and mechanical properties, so microstructure ...
Zhanguang Zheng   +4 more
doaj   +1 more source

Investigating accidents involving aircraft manufactured from polymer composite materials [PDF]

open access: yes, 2013
This thesis looks into the examination of polymer composite wreckage from the perspective of the aircraft accident investigator. It develops an understanding of the process of wreckage examination as well as identifying the potential for visual and ...
Dunn, Leigh
core  

Correlative light-electron fractography for fatigue striations characterization in metallic alloys

open access: yes, 2013
The correlative light-electron fractography technique combines correlative microscopy concepts to the extended depth-from-focus reconstruction method, associating the reliable topographic information of 3-D maps from light microscopy ordered Z-stacks to ...
Campos, Kamila Amato de   +8 more
core   +1 more source