Results 111 to 120 of about 5,991 (129)

ADM guidance—Ceramics: guidance to the use of fractography in failure analysis of brittle materials

open access: yesDental Materials, 2017
Objectives. To provide background information and guidance as to how to use fractographyaccurately, a powerful tool for failure analysis of dental ceramic structures. Methods.
Paulo Francisco Cesar   +2 more
exaly   +2 more sources

Formability Limits, Fractography and Fracture Toughness in Sheet Metal Forming

open access: yesMaterials, 2019
This paper is focused on the utilisation of double edge notched tension, staggered and shear tests to determine fracture toughness and the formability limits by fracture in principal strain space.
Luis Reis   +2 more
exaly   +2 more sources
Some of the next articles are maybe not open access.

Related searches:

Quantitative fractography for brittle fracture via multilayer perceptron neural network

Engineering Fracture Mechanics, 2023
Lingyue Ma   +2 more
exaly  

Formability and fractography of AA5754/polyethylene/AA5754 sandwich composites

Mechanics Based Design of Structures and Machines, 2022
Ramin Hashemi, Seyed Ali Niknam
exaly  

Forensic fractography of bone using computed tomography (CT) scans

Journal of Forensic Radiology and Imaging, 2019
Gary M Hatch
exaly  

Quantitative fractography of fatigue and an illustrative case study

Engineering Failure Analysis, 2019
Loris Molent
exaly  

Fractography of self-glazed zirconia with improved reliability

Journal of the European Ceramic Society, 2017
Mirva Eriksson   +2 more
exaly  

Home - About - Disclaimer - Privacy