Results 141 to 150 of about 6,333 (218)
Influence of ageing time on the microstructural and mechanical behaviour of Al-Si-Mg/coconut shell ash metal matrix composite. [PDF]
Murali AP +7 more
europepmc +1 more source
Mechanical performance and microstructural behavior of ultrasonically welded PVC-coated polyester fabric seams at subzero temperature. [PDF]
Eskandarnia G +3 more
europepmc +1 more source
Polar Cryogenic Impact Behavior of Selective Laser Melted Ti-6Al-4V Alloy: Effects of Scanning Strategies and Notch Orientation. [PDF]
Chen H +6 more
europepmc +1 more source
Pre-weld friction stir processing mitigates hot cracking and strengthens AA6061 fusion welds. [PDF]
Jalili A +4 more
europepmc +1 more source
Study on the Transverse Properties of T800-Grade Unidirectional Carbon Fiber-Reinforced Polymers. [PDF]
Wang H +9 more
europepmc +1 more source
openaire +1 more source
Tailoring Microstructure and Performance of Cu/SiC Composites via Integrated Powder Metallurgy and Thermo-Compression Processing. [PDF]
Shan M +6 more